Nanoindentation of Porous Bulk and Thin Films of LSCF

Abstract

In this paper we show how reliable measurements on porous ceramic films can be made by appropriate nanoindentation experiments and analysis. Room-temperature mechanical properties of the mixed-conducting perovskite material LSCF6428 were investigated by nanoindentation of porous bulk samples and porous films sintered at temperatures from 900-1200C. A spherical indenter was used so that the contact area was much greater than the scale of the porous microstructure. The elastic modulus of the bulk samples was found to increase from 33.8-174.3 GPa and hardness from 0.64-5.32 GPa as the porosity decreased from 45-5% after sintering at 900-1200C. Densification under the indenter was found to have little influence on the measured elastic modulus. The residual porosity in the dense sample was found to account for the discrepancy between the elastic moduli measured by indentation and by impulse excitation. Crack-free LSCF6428 films of acceptable surface roughness for indentation were also prepared by sintering at 900-1200C. Reliable measurements of the true properties of the films were obtained by data extrapolation provided that the ratio of indentation depth to film thickness was in the range 0.1 to 0.2. The elastic moduli of the films and bulk materials were approximately equal for a given porosity. The 3D microstructures of films before and after indentation were characterized using FIB-SEM tomography. Finite element modelling of the elastic deformation of the actual microstructures showed excellent agreement with the nanoindentation results.

Explore related subjects

Keep this discovery

BibTeXRIS

Zhangwei Chen, Xin Wang, Vinnet Bhakhri, Finn Giuliani, Alan Atkinson. 2015-02-07. Nanoindentation of Porous Bulk and Thin Films of LSCF. https://doi.org/10.1016/j.actamat.2013.06.016

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.

cond-mat.mtrl-sci