Improved room-temperature-selectivity between Nd and Fe in Nd recovery from Nd-Fe-B magnet
Abstract
The sustainable society requires the recycling of rare metals. Rare earth Nd is one of rare metals, accompanying huge consumption especially in Nd-Fe-B magnets. Although the wet process using acid is in practical use in the in-plant recycle of sludge, higher selectivity between Nd and Fe at room temperature is desired. We have proposed a pretreatment of corrosion before the dissolution into HCl and the oxalic acid precipitation. The corrosion produces $γ$-FeOOH and a Nd hydroxide, which have high selectivity for HCl solution at room temperature. Nd can be recovered as Mn$_{2}$O$_{3}$-type Nd$_{2}$O$_{3}$. The estimated recovery-ratio of Nd reaches to 97\%.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Yusuke Kataoka, Taisuke Ono, Masami Tsubota, Jiro Kitagawa. 2015-11-01. Improved room-temperature-selectivity between Nd and Fe in Nd recovery from Nd-Fe-B magnet. https://arxiv.org/abs/1511.00325
Cite the original work for its findings. Save a collection to share your selection of sources.