SearcharxivSearch

arXiv · 1603.05081

Criteria for extensional necking instability in complex fluids and soft solids. Part I: imposed Hencky strain rate protocol

Abstract

We study the necking dynamics of a filament of complex fluid or soft solid in uniaxial tensile stretching at constant imposed Hencky strain rate $\dot\varepsilon$, by means of linear stability analysis and nonlinear (slender filament) simulations. We demonstrate necking to be an intrinsic flow instability that arises as an inevitable consequence of the constitutive behaviour of essentially any material (with a possible rare exception, which we outline). We derive criteria for the onset of necking that are reportable simply in terms of characteristic signatures in the shapes of the experimentally measured rheological response functions, and should therefore apply universally to all materials. As evidence of their generality, we numerically show them to hold in six popular constitutive models of polymers and soft glasses. Two distinct modes of necking instability are predicted. The first is relatively gentle, and sets in when the tensile stress signal first curves down as a function of the time $t$ (or accumulated strain $\epsilon=\dot\varepsilon t$) since the inception of the flow. The second is more violent, and sets in when a carefully defined `elastic derivative' of the tensile force first slopes down as a function of $t$ (or $\dot\varepsilon$). In the limit of fast flow $\dot\varepsilon\tau\to\infty$, where $\tau$ is the material's characteristic stress relaxation time, this second mode reduces to the Consid\'ere criterion for necking in solids. However we show that the Consid\'ere criterion fails to correctly predict the onset of necking in any viscoelastic regime of finite imposed $\dot\varepsilon\tau$. Finally, we elucidate the way these modes of instability manifest themselves in entangled linear polymers, wormlike micelles and branched polymers. We demonstrate four distinct regimes as a function of imposed strain rate, consistent with experimental master curves.

Explore related subjects

Keep this discovery

BibTeXRIS

David M. Hoyle, Suzanne M. Fielding. 2016-03-16. Criteria for extensional necking instability in complex fluids and soft solids. Part I: imposed Hencky strain rate protocol. https://doi.org/10.1122/1.4965036

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Slow Dynamics and the Geometry of Jammed Packings

Saddle points in the energy landscape of granular packings dominate the discrete steepest descent dynamics and ultimately determine the path that an out of mechanical equilibrium packing will follow and the resulting stable minimum that it will find. The saddle points that ultimately determine the resulting minima tend to be low-index saddle points. For models with an analytic energy landscape, such as the $p$-spin model, the steepest descent minimization path is affected by higher-index saddle points, which pull the system towards saddle points of decreasing index before arriving at the minima. Here, we examine the steepest descent minimization path of granular packings and compare them to the $p$-spin model. We show that the granular packing steepest descent minimization paths act like their smooth energy landscape counterparts and get attracted by saddle points. The index versus time curves for all models follow a shifted, stretched exponential. We further show that the shape parameter for the granular packings is unchanged when the energy landscape is modified to become analytic (Gaussian potential in a harmonic well) or non-local (Mari-Krzakala-Kurchan). The $p$-spin, on the other hand, has a significantly larger shape parameter. The reason is not due to the dimensionality, packing fraction, nonanalyticity, or the locality of the Hamiltonian of the models. The exact reason for the discrepancy in the shape parameter is \st{still} an unsolved mystery.

cond-mat.soft

A Phase-Field Study of Desiccation Crack Pattern Maturation under Drying-Wetting Cycles

The characteristic intersection angle of the desiccation crack relaxes from near \ang{90} toward \ang{120} under repeated drying--wetting cycles. However, the theoretical understanding of this relaxation is insufficient, especially the modeling of the drying--wetting cycles. Here we introduce a phase-field model of desiccation fracture, extending the model proposed in previous studies by adding crack healing and a scar effect left by past cracks. By repeating drying--wetting cycles in a finite element simulation, we find that the angle distribution develops a growing peak near \ang{120} as the cycle number increases, consistent with experiments. The standard deviation of the intersection angle from \ang{120} relaxes exponentially with a characteristic time of about 2.85 cycles. These results are consistent with experiments, except that the characteristic time is slightly smaller than the experimental value. Crack energy dominates the total energy and also relaxes exponentially with nearly the same characteristic cycle as the angle relaxation. This decay is driven mainly by a shortening of the effective crack length rather than a change in effective fracture toughness.

cond-mat.soft

Kinetics of ferritin crystal formation and melting in acoustically levitated droplets

Understanding protein crystallization pathways is essential for controlling crystallization in structural biology, materials science, and pharmaceutical applications. Classical nucleation theory does not fully capture crystallization processes for several proteins, including ferritin. Here, we combine acoustic levitation with small- and wide-angle X-ray scattering (SAXS and WAXS) to monitor ferritin crystallization in evaporating aqueous polyethylene glycol (PEG) solutions. Acoustic levitation rapidly drives the droplets through a broad range of protein and polymer concentrations, enabling time-resolved measurements of crystallization during evaporation. The scattering data show that ferritin crystals form during evaporation and subsequently lose their crystalline order upon further dehydration. Varying the PEG molecular weight switches between distinct crystallization pathways: one dominated by attractive protein-protein interactions and another dominated by repulsive interactions and excluded-volume effects. Furthermore, we find that lower molecular weight PEG (1000 g/mol) suppresses the dehydration-induced loss of crystalline order observed for higher molecular weight PEG (6000 g/mol), providing a simple strategy for improving protein crystal stability.

cond-mat.soft