arXiv · 1712.09385
Thermoelectric Power of the CeCoAl$_4$ Antiferromagnet - Predominance of the Crystal Electric Field
Abstract
We report on the thermoelectric power $S(T)$, electrical resistivity and thermal conductivity measurements on the antiferromagnetic CeCoAl$_4$ compound. The N\'eel temperature of CeCoAl$_4$ is $T_N$=13.5K and a metamagnetic-like transition occurs in the magnetic field of about 7.5T. We show that the magnetic contribution to the thermoelectric power, $S_f(T)$, exhibits a large peak due to the crystal electric field (CEF) at about 240K and a small anomaly around the ordering temperature. Surprisingly, the CEF related $S_f(T)$ peak is close to the upper CEF excitation energy $\Delta_2$=202K, in contrast to the usual case of the peak position being a fraction of the real CEF excitation. The applicability of different theoretical and phenomenological models describing the temperature dependence of the Seebeck effect $S_f(T)$ has been tested and finally a calculation is proposed, which incorporates a full CEF levels scheme. For the nonmagnetic reference compound, LaCoAl$_4$, the thermoelectric power measurements provide an evidence of the phonon drag contribution, which is not present or masked in the case of CeCoAl$_4$.
Explore related subjects
Keep this discovery
Tomasz Toliński. 2017-12-26. Thermoelectric Power of the CeCoAl$_4$ Antiferromagnet - Predominance of the Crystal Electric Field. https://arxiv.org/abs/1712.09385
Cite the original work for its findings. Save a collection to share your selection of sources.