arXiv · 1808.10763
On the miscibility gap at 800 K in the Fe-Cr alloy system
Abstract
Issues pertinent to the miscibility gap at 800K in a Fe73.7Cr26.3 alloy viz. the kinetics of the phase decomposition and borders of the latter were investigated by means of the Mössbauer-effect spectroscopy. The kinetics was revealed to well follow the Johnson-Mehl-Avrami-Kolgomarov equation testifying to a nucleation and growth mechanism underlying the decomposition. A solubility limit of Cr in the Fe matrix was determined to be 17.3(6) at.% and that of Fe in the Cr matrix was found as equal to 18.5(9) at.%. The results obtained have been compared with various theoretical predictions.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Stanislaw M. Dubiel, Jan Zukrowski. 2018-08-31. On the miscibility gap at 800 K in the Fe-Cr alloy system. https://doi.org/10.1088/2053-1591%2Faaf18d
Cite the original work for its findings. Save a collection to share your selection of sources.