Effect of bed temperature on solute segregation and mechanical properties in Ti-6Al-4V produced by selective laser melting
Abstract
Advanced characterisation techniques were used on LPBF Ti-6Al-4V samples produced on a heated base plate. When the substrate temperature is 100{\deg}C the elongation is 6\%, which increases and peaks at 10\% at 570{\deg}C, then sharply decreases to zero ductility at 770{\deg}C. At 100{\deg}C, a heavily strained and twinned microstructure, primarily composed of {\alpha}+{\alpha}', was observed and it was comparable to asbuilt microstructures obtained by conventional LPBF methods. At higher temperatures, twins are no longer present and instead nano-scale {\beta} precipitates are observed within {\alpha}' and {\alpha}, as well as dislocation networks (570{\deg}C) and tangles (770{\deg}C). Solute segregation at crystal defects was observed in all pre-heating conditions. Al and V segregation at microtwins was observed in the 100{\deg}C sample, reporting for the first time `selective' and mutually exclusive Al- and V-rich regions forming in adjacent twins. V segregation at dislocations was observed in the 570{\deg}C and 770{\deg}C samples, consistent with the higher preheating temperatures. High O contents were measured in all samples but with apparent opposing effects. At 100{\deg}C and 570{\deg}C was estimated to be below the critical threshold for O embrittlement and locally aids in maintaining a strength high by solid solution strengthening, whereas at 770{\deg}C it was above the threshold, therefore failing in a brittle fashion. Based on these observations, the initial increase in ductility from 100{\deg}C to 570{\deg}C is attributed to a reduction in microtwins and the dislocation networks acting as `soft barriers' for slip within a coarser microstructure. The lack of ductility at 770{\deg}C was attributed to local solute redistribution causing dislocation pinning and an increase of O content in this sample.
Explore related subjects
Keep this discovery
S. Pedrazzini, M. E. Pek, A. K. Ackerman, Q. Cheng, H. Ali, H. Ghadbeigi, K. Mumtaz, T. Dessolier, T. B. Britton, P. Bajaj, E. Jägle, B. Gault, A. J. London, E. Galindo-Nava. 2020-06-15. Effect of bed temperature on solute segregation and mechanical properties in Ti-6Al-4V produced by selective laser melting. https://arxiv.org/abs/2006.08288
Cite the original work for its findings. Save a collection to share your selection of sources.