arXiv · 2112.08719
Environment-assisted crack nucleation in La(Fe,Mn,Si)13-based magnetocaloric materials
Abstract
Cracking in La(Fe,Si)13-based magnetocaloric materials has been observed to predominantly form around La-rich (La2O3) particles and pose a threat to their long-term structural integrity. To understand the formation of these cracks, FIB cross-sectional polishing followed by SEM characterisation was employed to study local microstructural evolution after air exposure. Results suggest that volume expansion and internal degradation associated with a chemical reaction between La2O3 particles and water/moisture can lead to crack nucleation in the 1:13 phase adjacent to La-rich particles. This observation indicates that the formation of La-rich phase should be suppressed, or their size minimised during material processing to ensure the long-term structural integrity of La(Fe,Mn,Si)13 magnetocaloric materials.
Explore related subjects
Keep this discovery
Siyang Wang, Edmund Lovell, Liya Guo, Neil Wilson, Mary P. Ryan, Finn Giuliani. 2021-12-16. Environment-assisted crack nucleation in La(Fe,Mn,Si)13-based magnetocaloric materials. https://arxiv.org/abs/2112.08719
Cite the original work for its findings. Save a collection to share your selection of sources.