Tuning the dynamics of chiral domain walls of ferrimagnetic films with the magneto-ionic effect

Abstract

The manipulation of magnetism with a gate voltage is expected to lead the way towards the realization of energy-efficient spintronics devices and high-performance magnetic memories. Exploiting magneto-ionic effects under micro-patterned electrodes in solid-state devices adds the possibility to modify magnetic properties locally, in a non-volatile and reversible way. Tuning magnetic anisotropy, magnetization and Dzyaloshinskii-Moriya interaction allows modifying at will the dynamics of non trivial magnetic textures such as skyrmions and chiral domain walls in magnetic race tracks. In this work, we illustrate efficient magneto-ionic effects in a ferrimagnetic Pt/Co/Tb stack using a ZrO2 thin layer as a solid state ionic conductor. When a thin layer of terbium is deposited on top of cobalt, it acquires a magnetic moment that aligns antiparallel to that of cobalt, reducing the effective magnetization. Below the micro-patterned electrodes, the voltage-driven migration of oxygen ions in a ZrO2 towards the ferrimagnetic stack partially oxidizes the Tb layer, leading to the local variation not only of the spontaneous magnetization, but also of the effective magnetic anisotropy and of the Dzyaloshinskii-Moriya interaction. This leads to a huge increase of the domain wall velocity, which varies from 10 m/s in the pristine state to 250 m/s after gating. This non-volatile and reversible tuning of the domain wall dynamics may lead to applications to reprogrammable magnetic memories or other spintronic devices.

Explore related subjects

Keep this discovery

BibTeXRIS

Cristina Balan, Jose Pena Garcia, Aymen Fassatoui, Jan Vogel, Dayane de Souza Chaves, Marlio Bonfim, Jean-Pascal Rueff, Laurent Ranno, Stefania Pizzini. 2022-05-06. Tuning the dynamics of chiral domain walls of ferrimagnetic films with the magneto-ionic effect. https://doi.org/10.1103/physrevapplied.18.034065

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.

cond-mat.mtrl-sci