SearcharxivSearch

arXiv · 2304.12104

Data-driven rheological characterization of stress buildup and relaxation in thermal greases

Abstract

Thermal greases, often used as thermal interface materials, are complex paste-like mixtures composed of a base polymer in which dense metallic (or ceramic) filler particles are dispersed to improve the heat transfer properties of the material. They have complex rheological properties that impact the performance of the thermal interface material over its lifetime. We perform rheological experiments on thermal greases and observe both stress relaxation and stress buildup regimes. This time-dependent rheological behavior of such complex fluid-like materials is not captured by steady shear-thinning models often used to describe these materials. We find that thixo-elasto-visco-plastic (TEVP) and nonlinear-elasto-visco-plastic (NEVP) constitutive models characterize the observed stress relaxation and buildup regimes respectively. Specifically, we use the models within a data-driven approach based on physics-informed neural networks (PINNs). PINNs are used to solve the inverse problem of determining the rheological model parameters from the dynamic response in experiments. This training data is generated by startup flow experiments at different (constant) shear rates using a shear rheometer. We validate the ``learned'' models by comparing their predicted shear stress evolution to experiments under shear rates not used in the training datasets. We further validate the learned TEVP model by solving a forward problem numerically to determine the shear stress evolution for an input step-strain profile. Meanwhile, the NEVP model is further validated by comparison to a steady Herschel--Bulkley fit of the material's flow curve.

Explore related subjects

Keep this discovery

BibTeXRIS

Pranay P. Nagrani, Ritwik V. Kulkarni, Parth U. Kelkar, Ria D. Corder, Kendra A. Erk, Amy M. Marconnet, Ivan C. Christov. 2023-04-24. Data-driven rheological characterization of stress buildup and relaxation in thermal greases. https://doi.org/10.1122/8.0000679

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Slow Dynamics and the Geometry of Jammed Packings

Saddle points in the energy landscape of granular packings dominate the discrete steepest descent dynamics and ultimately determine the path that an out of mechanical equilibrium packing will follow and the resulting stable minimum that it will find. The saddle points that ultimately determine the resulting minima tend to be low-index saddle points. For models with an analytic energy landscape, such as the $p$-spin model, the steepest descent minimization path is affected by higher-index saddle points, which pull the system towards saddle points of decreasing index before arriving at the minima. Here, we examine the steepest descent minimization path of granular packings and compare them to the $p$-spin model. We show that the granular packing steepest descent minimization paths act like their smooth energy landscape counterparts and get attracted by saddle points. The index versus time curves for all models follow a shifted, stretched exponential. We further show that the shape parameter for the granular packings is unchanged when the energy landscape is modified to become analytic (Gaussian potential in a harmonic well) or non-local (Mari-Krzakala-Kurchan). The $p$-spin, on the other hand, has a significantly larger shape parameter. The reason is not due to the dimensionality, packing fraction, nonanalyticity, or the locality of the Hamiltonian of the models. The exact reason for the discrepancy in the shape parameter is \st{still} an unsolved mystery.

cond-mat.soft

A Phase-Field Study of Desiccation Crack Pattern Maturation under Drying-Wetting Cycles

The characteristic intersection angle of the desiccation crack relaxes from near \ang{90} toward \ang{120} under repeated drying--wetting cycles. However, the theoretical understanding of this relaxation is insufficient, especially the modeling of the drying--wetting cycles. Here we introduce a phase-field model of desiccation fracture, extending the model proposed in previous studies by adding crack healing and a scar effect left by past cracks. By repeating drying--wetting cycles in a finite element simulation, we find that the angle distribution develops a growing peak near \ang{120} as the cycle number increases, consistent with experiments. The standard deviation of the intersection angle from \ang{120} relaxes exponentially with a characteristic time of about 2.85 cycles. These results are consistent with experiments, except that the characteristic time is slightly smaller than the experimental value. Crack energy dominates the total energy and also relaxes exponentially with nearly the same characteristic cycle as the angle relaxation. This decay is driven mainly by a shortening of the effective crack length rather than a change in effective fracture toughness.

cond-mat.soft

Kinetics of ferritin crystal formation and melting in acoustically levitated droplets

Understanding protein crystallization pathways is essential for controlling crystallization in structural biology, materials science, and pharmaceutical applications. Classical nucleation theory does not fully capture crystallization processes for several proteins, including ferritin. Here, we combine acoustic levitation with small- and wide-angle X-ray scattering (SAXS and WAXS) to monitor ferritin crystallization in evaporating aqueous polyethylene glycol (PEG) solutions. Acoustic levitation rapidly drives the droplets through a broad range of protein and polymer concentrations, enabling time-resolved measurements of crystallization during evaporation. The scattering data show that ferritin crystals form during evaporation and subsequently lose their crystalline order upon further dehydration. Varying the PEG molecular weight switches between distinct crystallization pathways: one dominated by attractive protein-protein interactions and another dominated by repulsive interactions and excluded-volume effects. Furthermore, we find that lower molecular weight PEG (1000 g/mol) suppresses the dehydration-induced loss of crystalline order observed for higher molecular weight PEG (6000 g/mol), providing a simple strategy for improving protein crystal stability.