Polyelectrolytes in Solution and at Surfaces

Abstract

This chapter deals with charged polymers (polyelectrolytes) in solution and at surfaces. The behavior of polyelectrolytes is markedly different from that of neutral polymers. In bulk solutions, i.e. disregarding the surface effect, there are two unique features to charged polymers: first, due to the presence of long-ranged electrostatic repulsion between charged monomers, the polymer conformations are much more extended, giving rise to a very small overlap concentration and high solution viscosity. Second, the presence of a large number of counter-ions increases the osmotic pressure of polyelectrolyte solutions, making such polymers water soluble as is of great importance to many applications. At surfaces, the same interplay between monomer-monomer repulsion and counter-ion degrees of freedom leads to a number of special properties. In particular, the adsorption behavior depends on both the concentration of polymers and added salt in the bulk. We first describe the adsorption behavior of single polyelectrolyte molecules, and discuss the necessary conditions to obtain an adsorbed layer and characterize its width. Depending on the stiffness of the polyelectrolyte, the layer can be flat and compressed or coiled and extended. We then proceed and discuss the adsorption of polyelectrolytes from semi-dilute solutions. Mean-field theory profiles of polyelectrolyte adsorption are calculated as function of surface charge density (or surface potential), the amount of salt in the system and the charge fraction on the chains. The phenomenon of charge inversion is reviewed and its relevance to the formation of multilayers is explained. The review ends with a short overview of the behavior of grafted polyelectrolytes.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Roland R. Netz, David Andelman. 2001-09-25. Polyelectrolytes in Solution and at Surfaces. https://arxiv.org/abs/cond-mat/0101314

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Slow Dynamics and the Geometry of Jammed Packings

Saddle points in the energy landscape of granular packings dominate the discrete steepest descent dynamics and ultimately determine the path that an out of mechanical equilibrium packing will follow and the resulting stable minimum that it will find. The saddle points that ultimately determine the resulting minima tend to be low-index saddle points. For models with an analytic energy landscape, such as the $p$-spin model, the steepest descent minimization path is affected by higher-index saddle points, which pull the system towards saddle points of decreasing index before arriving at the minima. Here, we examine the steepest descent minimization path of granular packings and compare them to the $p$-spin model. We show that the granular packing steepest descent minimization paths act like their smooth energy landscape counterparts and get attracted by saddle points. The index versus time curves for all models follow a shifted, stretched exponential. We further show that the shape parameter for the granular packings is unchanged when the energy landscape is modified to become analytic (Gaussian potential in a harmonic well) or non-local (Mari-Krzakala-Kurchan). The $p$-spin, on the other hand, has a significantly larger shape parameter. The reason is not due to the dimensionality, packing fraction, nonanalyticity, or the locality of the Hamiltonian of the models. The exact reason for the discrepancy in the shape parameter is \st{still} an unsolved mystery.

cond-mat.soft

A Phase-Field Study of Desiccation Crack Pattern Maturation under Drying-Wetting Cycles

The characteristic intersection angle of the desiccation crack relaxes from near \ang{90} toward \ang{120} under repeated drying--wetting cycles. However, the theoretical understanding of this relaxation is insufficient, especially the modeling of the drying--wetting cycles. Here we introduce a phase-field model of desiccation fracture, extending the model proposed in previous studies by adding crack healing and a scar effect left by past cracks. By repeating drying--wetting cycles in a finite element simulation, we find that the angle distribution develops a growing peak near \ang{120} as the cycle number increases, consistent with experiments. The standard deviation of the intersection angle from \ang{120} relaxes exponentially with a characteristic time of about 2.85 cycles. These results are consistent with experiments, except that the characteristic time is slightly smaller than the experimental value. Crack energy dominates the total energy and also relaxes exponentially with nearly the same characteristic cycle as the angle relaxation. This decay is driven mainly by a shortening of the effective crack length rather than a change in effective fracture toughness.

cond-mat.soft

Kinetics of ferritin crystal formation and melting in acoustically levitated droplets

Understanding protein crystallization pathways is essential for controlling crystallization in structural biology, materials science, and pharmaceutical applications. Classical nucleation theory does not fully capture crystallization processes for several proteins, including ferritin. Here, we combine acoustic levitation with small- and wide-angle X-ray scattering (SAXS and WAXS) to monitor ferritin crystallization in evaporating aqueous polyethylene glycol (PEG) solutions. Acoustic levitation rapidly drives the droplets through a broad range of protein and polymer concentrations, enabling time-resolved measurements of crystallization during evaporation. The scattering data show that ferritin crystals form during evaporation and subsequently lose their crystalline order upon further dehydration. Varying the PEG molecular weight switches between distinct crystallization pathways: one dominated by attractive protein-protein interactions and another dominated by repulsive interactions and excluded-volume effects. Furthermore, we find that lower molecular weight PEG (1000 g/mol) suppresses the dehydration-induced loss of crystalline order observed for higher molecular weight PEG (6000 g/mol), providing a simple strategy for improving protein crystal stability.

cond-mat.soft