Temperature-induced barium de-trapping from a double-well potential in Ba6Ge25

Abstract

The crystal structure of barium-germanium clathrate Ba6Ge25 was studied using neutron powder diffraction in the temperature range 20-300K. The compound was found to be cubic (S.G. P4_1 23) in the entire temperature range. However, the fully-ordered model of the crystal structure (no split sites) is marginal at room temperature, and clearly fails at low temperature. A much better description of the crystal structure below 250K is given in terms of two split Ba sites, with random occupancies, for two out of three types of cages present in the Ba6Ge25 structure. The Ba atoms were found to interact strongly with the Ge host. The separation of the split Ba sites grows with decreasing temperature, with a sudden increase on cooling through the 200-250K temperature range, accompanied by an expansion of the entire crystal structure. We propose a simple model for this transition, based on temperature-induced de- trapping of Ba from a deep double-well potential. This transition is associated with sizeable anomalies in the transport and magnetic properties. The most significant of these effects, that is, the drop in electrical conductivity on cooling, can be easily explained within our model through the enhanced structural disorder, which would affect the relaxation time for all portions of the Fermi surface. We suggest that the other anomalies (increase in the absolute value of the negative Seebeck coefficient, decrease in the magnetic susceptibility) can be explained within the framework of the one-electron semi- classical model, without any need to invoke exotic electron-electron interaction mechanisms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

M. Schmidt, P. G. Radaelli, M. J. Gutmann, S. J. L. Billinge, N. Hur, S. W. Cheong. 2003-03-13. Temperature-induced barium de-trapping from a double-well potential in Ba6Ge25. https://doi.org/10.1088/0953-8984%2F16%2F41%2F010

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.