Enhanced thermopower in an intergrowth cobalt oxide Li$_{0.48}$Na$_{0.35}$CoO$_{2}$
Abstract
We report the measurements of thermopower, electrical resistivity and thermal conductivity in a complex cobalt oxide Li$_{0.48}$Na$_{0.35}$CoO$_{2}$, whose crystal structure can be viewed as an intergrowth of the O3 phase of Li$_{x}$CoO$_{2}$ and the P2 phase of Na$_{y}$CoO$_{2}$ along the c axis. The compound shows large room-temperature thermopower of $\sim$180 $μ$V/K, which is substantially higher than those of Li$_{x}$CoO$_{2}$ and Na$_{y}$CoO$_{2}$. The figure of merit for the polycrystalline sample increases rapidly with increasing temperature, and it achieves nearly 10$^{-4}$ K$^{-1}$ at 300 K, suggesting that Li$_{x}$Na$_{y}$CoO$_{2}$ system is a promising candidate for thermoelectric applications.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Zhi Ren, Jingqin Shen, Shuai Jiang, Xiaoyang Chen, Chunmu Feng, Zhu'an Xu, Guanghan Cao. 2005-11-29. Enhanced thermopower in an intergrowth cobalt oxide Li$_{0.48}$Na$_{0.35}$CoO$_{2}$. https://doi.org/10.1088/0953-8984%2F18%2F29%2Fl01
Cite the original work for its findings. Save a collection to share your selection of sources.