arXiv · cond-mat/0602402
Enhancement of JC-B Properties in MoSi2 doped MgB2 tapes
Abstract
MoSi2 doped MgB2 tapes with different doping levels were prepared through the in-situ powder-in-tube method using Fe as the sheath material. Effect of MoSi2 doping on the MgB2/Fe tapes was investigated. It is found that the highest JC value was achieved in the 2.5 at.% doped samples, more than a factor of 4 higher compared to the undoped tapes at 4.2 K, 10 T, then further increasing the doping ratio caused a reduction of JC. Moreover, all doped tapes exhibited improved magnetic field dependence of Jc. The enhancement of JC-B properties in MoSi2 doped MgB2 tapes is attributed to good grain linkage and the introduction of effective flux pining centers with the doping.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Xianping Zhang, Yanwei Ma, Zhaoshun Gao, Zhengguang Yu, G. Nishijima, K. Watanabe. 2006-02-17. Enhancement of JC-B Properties in MoSi2 doped MgB2 tapes. https://doi.org/10.1088/0953-2048%2F19%2F8%2F003
Cite the original work for its findings. Save a collection to share your selection of sources.