arXiv · cond-mat/0611651
Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy
Abstract
Bulk ferromagnetic amorphous Fe-Ni-P-B alloys in rod shape were formed by a rapid solidification technique. The largest amorphous specimen prepared had a diameter of ~2.5 mm and the corresponding cooling rate for the glass formation of this alloy system in our experiment can be estimate to be around 492.4 K/s by the method of finite-difference numerical calculation. This value is on the same order of magnitude as the critical cooling rate Rc of Fe40Ni40P14B6 alloy estimated by the method of constructing the continuous-cooling-transformation (CCT) curve. It is indicated that the heterophase impurities have been eliminated well in our experiment.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Qiang Li. 2006-11-29. Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy. https://arxiv.org/abs/cond-mat/0611651
Cite the original work for its findings. Save a collection to share your selection of sources.