Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys
Abstract
Ferromagnetic bulk amorphous Fe40Ni40P14B6 alloy rods with a diameter of 1.2 mm can be prepared by means of a rapid quenching technique. If a fluxing technique is also used, amorphous rods with a diameter as large as 2.5 mm can be synthesized. The critical cooling rate Rc for the glass formation Fe40Ni40P14B6 is estimated to be on the order of 100 K.s-1
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Qiang Li. 2006-11-27. Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys. https://doi.org/10.1016/j.matlet.2006.02.054