Second-Order Raman Scattering in Exfoliated Black Phosphorus

Second-order Raman scattering has been extensively studied in carbon-based nanomaterials, \emph{e.g.} nanotube and graphene, because it activates normally forbidden Raman modes that are sensitive to crystal disorder, such as defects, dopants, strain, etc. The sp$^2$-hybridized carbon systems are, however, the exception among most nanomaterials, where first-order Raman processes usually dominate. Here we report the identification of four second-order Raman modes, named $D_1$, $D_1'$, $D_2$ and $D_2'$, in exfoliated black phosphorus (P(black)), an elemental direct-gap semiconductor exhibiting strong mechanical and electronic anisotropies. Located in close proximity to the $A^1_g$ and $A^2_g$ modes, these new modes dominate at an excitation wavelength of 633 nm. Their evolutions as a function of sample thickness, excitation wavelength, and defect density indicate that they are defect-activated and involve high-momentum phonons in a doubly-resonant Raman process. \emph{Ab initio} simulations of a monolayer reveal that the $D'$ and $D$ modes occur through intravalley scatterings with split contributions in the armchair and zigzag directions, respectively. The high sensitivity of these $D$ modes to disorder helps explaining several discrepancies found in the literature.

cond-mat.mtrl-sci↗

Spectral responsivity and photoconductive gain in thin film black phosphorus photodetectors

We have fabricated black phosphorus photodetectors and characterized their full spectral responsivity. These devices, which are effectively in the bulk thin film limit, show broadband responsivity ranging from <400 nm to the ~3.8 $μ$m bandgap. In the visible, an intrinsic responsivity >7 A/W can be obtained due to internal gain mechanisms. By examining the full spectral response, we identify a sharp contrast between the visible and infrared behavior. In particular, the visible responsivity shows a large photoconductive gain and gate-voltge dependence, while the infrared responsivity is nearly independent of gate voltage and incident light intensity under most conditions. This is attributed to a contribution from the surface oxide. In addition, we find that the polarization anisotropy in responsivity along armchair and zigzag directions can be as large as 103 and extends from the band edge to 500 nm. The devices were fabricated in an inert atmosphere and encapsulated by Al$_2$O$_3$ providing stable operation for more than 6 months.

physics.app-ph↗