Searcharxiv⌕ Search

arXiv subjects

D. A. Zotov

Publications and source records attributed to D. A. Zotov.

2 recordsLinked to original sources

Localized corrosion resistance of ultrafine-grained austenitic steel 321 obtained by Rotary Swaging: The role of annealing conditions

The object of this study was austenitic steel 321, which has an ultrafine-grained (UFG) structure formed by Rotary Swaging (RS). RS leads to the formation of a two-phase macroscopically heterogeneous and, at the same time, a microscopically homogeneous UFG structure with an increased content of martensite. It has been shown that secondary TiC nanoparticles form in the annealing at 450-550C, the reverse transformation of martensite into austenite occurs at 550-650C, and recrystallization begins at 700C. Electrochemical studies of the resistance of the UFG steel to general corrosion, intergranular corrosion (IGC), and pitting corrosion (PC) have been carried out. It has been shown that the UFG steel after RS has a reduced IGC resistance. The surface of steel rods after RS has a reduced hardness and corrosion resistance compared to the central part of the rods. It has been shown that in the temperature range of 450-550C, there is a slight increase in the microhardness, and a significant decrease in the IGC and PC resistance of the UFG steel. Recrystallization at 700-800C leads to an increased PC resistance and IGC resistance. Annealing conditions have been determined that ensure a good combination of strength, ductility and corrosion resistance of the UFG steel. It was demonstrated that to explain the non-monotonic variation in the localized corrosion rate of UFG steel during annealing, it is necessary to consider not only the well-known effects of martensite and delta-ferrite, but also the precipitation of TiC particles and the changes in the free energy of non-equilibrium grain boundaries.

cond-mat.mtrl-sci↗

Effect of superplastic deformation on the intergranular corrosion resistance of austenitic steel 321 with different types of UFG structure: A case of homogeneous and heterogeneous microstructure obtained by ECAP

The effects of superplasticity (SP) on the structure, hardness, and intergranular corrosion (IGC) resistance of UFG 321L steel are reported. By increasing the number of the ECAP cycles (N) and varying the ECAP temperature, and annealing temperature, the degree of the microstructural heterogeneity was changed. Regardless of the microstructural homogeneity degree, UFG steels demonstrated the possibility of realizing the SP effect at temperatures below the onset temperature of dynamic recrystallization. The dependence of ductility of the UFG steel on the test temperature is non-monotonic with a minimum at 450-600C. The maximum elongation to failure (~250%) was achieved at a SP temperature of 800C. The SP deformation of the UFG steel is controlled by the power law creep. It is shown that the hardness of UFG steel samples after SP is equal than the hardness of UFG steels annealed at the same temperature. It is also shown what SP leads to a decrease in the IGC resistance of the UFG steel. Heterostructured steel have reduced ductility, as well as lower resistance to IGC after tension tests at room temperature (RT). The minimum IGC resistance is ensured at N=2, and the maximum - at N=4. The IGC resistance of homogeneous UFG samples after tension testing exceeds the IGC resistance of coarse-grained steel. Tension test at a RT has the greatest negative effect on the IGC resistance of heterostructured steel, and the least negative effect on the IGC resistance of homogeneous steel. Increasing the number of ECAP cycles enhances the ductility of the UFG steel at 750-900C. Increasing the ECAP temperature results in a simultaneous decrease in ductility and flow stress. Heterostructured steel exhibits minimal values of the activation energy of SP deformation. Increasing the number of ECAP cycles and increasing the ECAP temperature lead to an increase in the activation energy of SP deformation.

cond-mat.mtrl-sci↗