SearcharxivSearch

arXiv subjects

E. Lundgren

Publications and source records attributed to E. Lundgren.

4 recordsLinked to original sources

Evidence for the Active Phase of Heterogeneous Catalysts through In Situ Reaction Product Imaging and Multiscale Modeling

We use multi-scale modeling to analyze laser-induced fluorescence (LIF) measurements of the CO oxidation reaction over Pd(100) at near-ambient reaction conditions. Integrating density-functional theory based kinetic Monte Carlo simulations of the active catalyst into fluid-dynamical simulations of the mass transport inside the reactor chamber we calculate the reaction product concentration directly above the catalyst surface. Comparing corresponding data calculated for different surface models against the measured LIF signals we can discriminate the one that predominantly actuates the experimentally measured catalytic activity. For the probed CO oxidation reaction conditions the experimental activity is due to pristine Pd(100), possibly coexisting with other (oxidic) domains on the surface.

cond-mat.mtrl-sci

In situ X-ray photoelectron spectroscopy of model catalysts: At the edge of the gap

We present a High-Pressure X-ray Photoelectron Spectroscopy (HP-XPS) and first-principles kinetic Monte Carlo study addressing the nature of the active surface in CO oxidation over Pd(100). Simultaneously measuring the chemical composition at the surface and in the near-surface gas-phase, we reveal both O-covered pristine Pd(100) and a surface oxide as stable, highly active phases in the near-ambient regime accessible to HP-XPS. Surprisingly, no adsorbed CO can be detected during high CO2 production rates, which can be explained by a combination of a remarkably short residence time of the CO molecule on the surface and mass-transfer limitations in the present set-up.

physics.chem-ph

Kinetic hindrance during the initial oxidation of Pd(100) at ambient pressures

The oxidation of the Pd(100) surface at oxygen pressures in the 10^-6 to 10^3 mbar range and temperatures up to 1000 K has been studied in-situ by surface x-ray diffraction (SXRD). The results provide direct structural information on the phases present in the surface region and on the kinetics of the oxide formation. Depending on the (T,p) environmental conditions we either observe a thin sqrt(5) x sqrt(5) R27 surface oxide or the growth of a rough, poorly ordered bulk oxide film of PdO predominantly with (001) orientation. By either comparison to the surface phase diagram from first-principles atomistic thermodynamics or by explicit time-resolved measurements we identify a strong kinetic hindrance to the bulk oxide formation even at temperatures as high as 675 K.

cond-mat.mtrl-sci

The Pd(100)-(SQRT(5) x SQRT(5) R27^o)-O surface oxide revisited

Combining high-resolution core-level spectroscopy (HRCLS), scanning tunneling microscopy (STM) and density-functional theory (DFT) calculations we reanalyze the Pd(100)-(SQRT(5) x SQRT(5) R27^o)-O surface oxide phase. We find that the prevalent structural model, a rumpled PdO(001) film suggested by previous low energy electron diffraction (LEED) work (M. Saidy et al., Surf. Sci. 494, L799 (2001)), is incompatible with all three employed methods. Instead, we suggest the two-dimensional film to consist of a strained PdO(101) layer on top of Pd(100). LEED intensity calculations show that this model is compatible with the experimental data of Saidy et al.

cond-mat.mtrl-sci