Towards establishing best practice in the analysis of hydrogen and deuterium by atom probe tomography

As hydrogen is touted as a key player in the decarbonization of modern society, it is critical to enable quantitative H analysis at high spatial resolution, if possible at the atomic scale. Indeed, H has a known deleterious impact on the mechanical properties (strength, ductility, toughness) of most materials that can hinder their use as part of the infrastructure of a hydrogen-based economy. Enabling H mapping, including local hydrogen concentration analyses at specific microstructural features, is essential for understanding the multiple ways that H affect the properties of materials, including for instance embrittlement mechanisms and their synergies, but also spatial mapping and quantification of hydrogen isotopes is essential to accurately predict tritium inventory of future fusion power plants, ensuring their safe and efficient operation for example. Atom probe tomography (APT) has the intrinsic capabilities for detecting hydrogen (H), and deuterium (D), and in principle the capacity for performing quantitative mapping of H within a material's microstructure. Yet the accuracy and precision of H analysis by APT remain affected by the influence of residual hydrogen from the ultra-high vacuum chamber that can obscure the signal of H from within the material, along with a complex field evaporation behavior. The present article reports the essence of discussions at a focused workshop held at the Max-Planck Institute for Sustainable Materials in April 2024. The workshop was organized to pave the way to establishing best practices in reporting APT data for the analysis of H. We first summarize the key aspects of the intricacies of H analysis by APT and propose a path for better reporting of the relevant data to support interpretation of APT-based H analysis in materials.

cond-mat.mtrl-sci↗

Optimizing site-specific specimen preparation for Atom Probe Tomography by using hydrogen for visualizing radiation-induced damage

Atom probe tomography (APT) is extensively used to measure the local chemistry of materials. Site-specific preparation via a focused ion beam (FIB) is routinely implemented to fabricate needle-shaped specimens with an end radius in the range of 50 nm. This preparation route is sometimes supplemented by transmission Kikuchi diffraction (TKD) to facilitate the positioning of a region of interest sufficiently close to the apex. Irradiating the specimen with energetic electrons and ions can lead to the generation of vacancies and even amorphization of the specimen. These extrinsically created vacancies become crucial for probing the hydrogen or deuterium distribution since they act as a strong trap. Here, we investigated the feasibility of site-specific preparation of a two-phase medium-Mn steel containing austenite (fcc) and ferrite (bcc). Following gaseous charging of APT specimens in deuterium (D2), clusters enriched by up to 35 at.% D, are imaged after Pt deposition, conventional Ga-FIB preparation, and TKD conducted separately. These D-rich clusters are assumed to arise from the agglomeration of vacancies acting as strong traps. By systematically eliminating these preparation-induced damages, we finally introduce a workflow allowing for studying intrinsic traps for H/D inherent to the material.

cond-mat.mtrl-sci↗

A new class of carbon stabilized austenitic steels resistant to hydrogen embrittlement

High strength steels are susceptible to H-induced failure, which is typically caused by the presence of diffusible H in the microstructure. The diffusivity of H in austenitic steels with fcc crystal structure is slow. The austenitic steels are hence preferred for applications in the hydrogen-containing atmospheres. However, the fcc structure of austenitic steels is often stabilized by the addition of Ni, Mn or N, which are relatively expensive alloying elements to use. Austenite can kinetically also be stabilized by using C. Here, we present an approach applied to a commercial cold work tool steel, where we use C to fully stabilize the fcc phase. This results in a microstructure consisting of only austenite and an M7C3 carbide. An exposure to H by cathodic hydrogen charging exhibited no significant influence on the strength and ductility of the C stabilized austenitic steel. While this material is only a prototype based on an existing alloy of different purpose, it shows the potential for low-cost H-resistant steels based on C stabilized austenite.

cond-mat.mtrl-sci↗

Atomic scale understanding of the role of hydrogen and oxygen segregation in the embrittlement of grain boundaries in a twinning induced plasticity steel

Twinning induced plasticity (TWIP) steels are high strength metallic materials with potential for structural components in e.g. automotive applications. However, they are prone to hydrogen embrittlement (HE) and galvanic corrosion. We investigated the susceptibility of a model Fe 27Mn 0.3C (wt%) TWIP steel towards HE and oxidation at the sub-nanometer scale by atom probe tomography. We measured segregation of hydrogen and oxygen at grain boundaries, which appears to be associated to a strong manganese depletion. Our study suggests a correlation between HE and oxidation mechanisms in TWIP steels, which we argue can combine to favor the previously reported hydrogen enhanced decohesion (HEDE) of grain boundaries.

cond-mat.mtrl-sci↗

Hydrogen-induced hardening of a high-manganese twinning induced plasticity steel

High-manganese twinning-induced plasticity (TWIP) steels exhibit high strain hardening, high tensile strength, and high ductility, which make them attractive for structural applications. At low tensile strain rates, TWIP steels are prone to hydrogen embrittlement (HE). Here though, we study the hardening and strengthening resulting from electrochemical hydrogen-charging of a surface layer of a Fe-26.9Mn-0.28C (wt.%) TWIP steel. We observed a 20% increase in yield strength following the electrochemical hydrogen-charging, accompanied by a reduction in ductility from 75% to 10% at a tensile strain rate of 10-3s-1. The microstructural evolution during tensile deformation was examined at strain levels of 3%, 5% and 7% by electron backscatter diffraction (EBSD) and electron channeling contrast imaging (ECCI) to study the dislocation structure of the hardened region. As expected, the microstructure of the hydrogen-hardened and the uncharged regions of the material evolve differently. The uncharged areas show entangled dislocation structures, indicating slip from a limited number of potentially coplanar slip systems. In contrast, hydrogen segregated to the grain boundaries, revealed by the deuterium-labelled atom probe tomography, delays the dislocation nucleation by blocking dislocation sources at the grain boundaries. The charged areas hence first show the formation of cells, indicating dislocation entanglement from more non-coplanar slip systems. With increasing strain, these cells dissolve, and stacking faults and strain-induced ε-martensite are formed, promoted by the presence of hydrogen. The influence of hydrogen on dislocation structures and the overall deformation mechanism is discussed in details.

cond-mat.mtrl-sci↗

Hydrogen embrittlement of twinning-induced plasticity steels: contribution of segregation to twin boundaries

Metallic materials, especially steel, underpin transportation technologies. High-manganese twinning induced plasticity (TWIP) austenitic steels exhibit exceptional strength and ductility from twins, low-energy microstructural defects that form during plastic loading. Their high-strength could help light-weighting vehicles, and hence cut carbon emissions. TWIP steels are however very sensitive to hydrogen embrittlement that causes dramatic losses of ductility and toughness leading to catastrophic failure of engineering parts. Here, we examine the atomic-scale chemistry and interaction of hydrogen with twin boundaries in a model TWIP steel by using isotope-labelled atom probe tomography, using tritium to avoid overlap with residual hydrogen. We reveal co-segregation of tritium and, unexpectedly, oxygen to coherent twin boundaries, and discuss their combined role in the embrittlement of these promising steels.

cond-mat.mtrl-sci↗

Transmission Kikuchi diffraction mapping induces structural damage in atom probe specimens

Measuring local chemistry of specific crystallographic features by atom probe tomography (APT) is facilitated by using transmission Kikuchi diffraction (TKD) to help position them sufficiently close to the apex of the needle-shaped specimen. However, possible structural damage associated to the energetic electrons used to perform TKD is rarely considered and is hence not well-understood. Here, in two case studies, we evidence damage in APT specimens from TKD mapping. First, we analyze a solid solution, metastable \b{eta}-Ti-12Mo alloy, in which the Mo is expected to be homogenously distributed. Following TKD, APT reveals a planar segregation of Mo amongst other elements. Second, specimens were prepared near Σ3 twin boundaries in a high manganese twinning-induced plasticity steel, and subsequently charged with deuterium gas. Beyond a similar planar segregation, voids containing a high concentration of deuterium, i.e. bubbles, are detected in the specimen on which TKD was performed. Both examples showcase damage from TKD mapping leading to artefacts in the compositional distribution of solutes. We propose that the structural damage is created by surface species, including H and C, subjected to recoil from incoming energetic electrons during mapping, thereby getting implanted and causing cascades of structural damage in the sample.

cond-mat.mtrl-sci↗

Laser-equipped gas reaction chamber for probing environmentally sensitive materials at near atomic scale

Numerous metallurgical and materials science applications depend on quantitative atomic-scale characterizations of environmentally-sensitive materials and their transient states. Studying the effect upon materials subjected to thermochemical treatments in specific gaseous atmospheres is of central importance for specifically studying a material's resistance to certain oxidative or hydrogen environments. It is also important for investigating catalytic materials, direct reduction of an oxide, particular surface science reactions or nanoparticle fabrication routes. This manuscript realizes such experiments upon a thermochemical reaction chamber called the Reacthub and allows for transferring treated materials under cryogenic & ultrahigh vacuum workflow conditions for characterisation by either atom probe or scanning Xe+/electron microscopies. Two examples are discussed in the present study. One protocol was in the deuterium gas charging (25 kPa D2 at 200 °C) of a high-manganese twinning-induced-plasticity steel and characterization of the ingress and trapping of hydrogen at various features (grain boundaries in particular) in efforts to relate this to the steel's hydrogen embrittlement susceptibility. Deuterium was successfully detected after gas charging but most contrast originated from the complex ion FeOD+ signal and the feature may be an artefact. The second example considered the direct deuterium reduction (5 kPa D2 at 700 °C) of a single crystal wuestite sample, demonstrating that under a standard thermochemical treatment causes rapid reduction upon the nanoscale. Further studies are required for complete confidence about these phenomena, but these experiments successfully demonstrate that how an ex-situ thermochemical treatment can be realised that captures environmentally-sensitive transient states that can be analysed by atomic-scale by atom probe microscope.

cond-mat.mtrl-sci↗

Hydrogen and deuterium charging of site-specific specimen for atom probe tomography

Hydrogen embrittlement can cause a dramatic deterioration of the mechanical properties of high-strength metallic materials. Despite decades of experimental and modelling studies, the exact underlying mechanisms behind hydrogen embrittlement remain elusive. To unlock understanding of the mechanism and thereby help mitigate the influence of hydrogen and the associated embrittlement, it is essential to examine the interactions of hydrogen with structural defects such as grain boundaries, dislocations and stacking faults. Atom probe tomography (APT) can, in principle, analyse hydrogen located specifically at such microstructural features but faces strong challenges when it comes to charging specimens with hydrogen or deuterium. Here, we describe three different workflows enabling hydrogen/deuterium charging of site-specific APT specimens: namely cathodic, plasma and gas charging. We discuss in detail the caveats of the different approaches in order to help with future research efforts and facilitate further studies of hydrogen in metals. Our study demonstrates successful cathodic and gas charging, with the latter being more promising for the analysis of the high-strength steels at the core of our work.

cond-mat.mtrl-sci↗