Localized corrosion resistance of ultrafine-grained austenitic steel 321 obtained by Rotary Swaging: The role of annealing conditions

The object of this study was austenitic steel 321, which has an ultrafine-grained (UFG) structure formed by Rotary Swaging (RS). RS leads to the formation of a two-phase macroscopically heterogeneous and, at the same time, a microscopically homogeneous UFG structure with an increased content of martensite. It has been shown that secondary TiC nanoparticles form in the annealing at 450-550C, the reverse transformation of martensite into austenite occurs at 550-650C, and recrystallization begins at 700C. Electrochemical studies of the resistance of the UFG steel to general corrosion, intergranular corrosion (IGC), and pitting corrosion (PC) have been carried out. It has been shown that the UFG steel after RS has a reduced IGC resistance. The surface of steel rods after RS has a reduced hardness and corrosion resistance compared to the central part of the rods. It has been shown that in the temperature range of 450-550C, there is a slight increase in the microhardness, and a significant decrease in the IGC and PC resistance of the UFG steel. Recrystallization at 700-800C leads to an increased PC resistance and IGC resistance. Annealing conditions have been determined that ensure a good combination of strength, ductility and corrosion resistance of the UFG steel. It was demonstrated that to explain the non-monotonic variation in the localized corrosion rate of UFG steel during annealing, it is necessary to consider not only the well-known effects of martensite and delta-ferrite, but also the precipitation of TiC particles and the changes in the free energy of non-equilibrium grain boundaries.

cond-mat.mtrl-sci↗

Effect of superplastic deformation on the intergranular corrosion resistance of austenitic steel 321 with different types of UFG structure: A case of homogeneous and heterogeneous microstructure obtained by ECAP

The effects of superplasticity (SP) on the structure, hardness, and intergranular corrosion (IGC) resistance of UFG 321L steel are reported. By increasing the number of the ECAP cycles (N) and varying the ECAP temperature, and annealing temperature, the degree of the microstructural heterogeneity was changed. Regardless of the microstructural homogeneity degree, UFG steels demonstrated the possibility of realizing the SP effect at temperatures below the onset temperature of dynamic recrystallization. The dependence of ductility of the UFG steel on the test temperature is non-monotonic with a minimum at 450-600C. The maximum elongation to failure (~250%) was achieved at a SP temperature of 800C. The SP deformation of the UFG steel is controlled by the power law creep. It is shown that the hardness of UFG steel samples after SP is equal than the hardness of UFG steels annealed at the same temperature. It is also shown what SP leads to a decrease in the IGC resistance of the UFG steel. Heterostructured steel have reduced ductility, as well as lower resistance to IGC after tension tests at room temperature (RT). The minimum IGC resistance is ensured at N=2, and the maximum - at N=4. The IGC resistance of homogeneous UFG samples after tension testing exceeds the IGC resistance of coarse-grained steel. Tension test at a RT has the greatest negative effect on the IGC resistance of heterostructured steel, and the least negative effect on the IGC resistance of homogeneous steel. Increasing the number of ECAP cycles enhances the ductility of the UFG steel at 750-900C. Increasing the ECAP temperature results in a simultaneous decrease in ductility and flow stress. Heterostructured steel exhibits minimal values of the activation energy of SP deformation. Increasing the number of ECAP cycles and increasing the ECAP temperature lead to an increase in the activation energy of SP deformation.

cond-mat.mtrl-sci↗

Effect of annealing on the hot salt corrosion resistance of the fine-grained titanium alpha-alloy Ti-2.5Al-2.6Zr obtained via cold Rotary Swaging

A hot salt corrosion (HSC) test was performed on the fine-grained titanium alpha-alloy Ti-2.5Al-2.6Zr (Russian industrial alloy PT-7M). The ultrafine-grained (UFG) microstructure in the titanium alpha-alloy was formed via cold Rotary Swaging. The grain size and volume fraction of the recrystallized microstructure in the alloy were varied by choosing appropriate annealing temperatures and times. The microstructure and corrosion resistance of UFG alloys were studied after 30 min of annealing at 500-700C and after 1000 h of annealing at 250C. Metallographic studies were carried out to investigate the effects of annealing on the nature and extent of corrosive damage in the titanium alpha-alloy Ti-2.5Al-2.6Zr. After HSC tests, surface analyses of the titanium alpha-alloy samples were conducted using X-ray diffraction and electron microscopy. During the HSC testing of the titanium alpha-alloy Ti-2.5Al-2.6Zr, a competitive interaction between intergranular corrosion (IGC) and pitting corrosion was observed. To the best of our knowledge, it was shown for the first time that annealing affects the relationship among the IGC, pitting corrosion and uniform corrosion rates of the titanium alloy. Prolonged low-temperature annealing at 250C resulted in a more pronounced increase in the uniform corrosion rate than short-term high-temperature annealing for 30 min at 500-700C. An in-depth analysis of the effect of the structure and phase composition of the grain boundaries on the susceptibility of the alpha-alloy Ti-2.5Al-2.6Zr to HSC was conducted.

physics.app-ph↗

Effect of annealing on the corrosion-fatigue strength and hot salt corrosion resistance of fine-grained titanium near-α alloy Ti-5Al-2V obtained by Rotary Swaging

The corrosion-fatigue strength in 3% aqueous NaCl solution and the resistance against hot salt corrosion (HSC) of the fine-grained near-a alloy Ti-5Al-2V (Russian analog of Grade 9 titanium alloy with increased aluminum content) has been studied. The properties of the Ti-5Al-2V alloy in the coarse-grained state, in the fine-grained after cold Rotary Swaging (RS), in partly recrystallized state, and in fully recrystallized one have been investigated. The mechanical properties of the alloy were characterized using compression tests and microhardness measurements. The effects of RS and of the annealing temperature and time on the character of corrosion destruction of the surface and on the composition of the products of the HSC were studied. RS was shown to result in an increase in the depth of the intergranular corrosion defects while the recrystallization annealing promotes the increasing of the corrosion resistance of the Ti-5Al-2V titanium alloy. The parameters of the Basquin equation for the corrosion-fatigue curves for the near-a Ti-5Al-2V alloy in the coarse-grained state, in the severely strained one, and after recrystallization annealing were determined for the first time. An effect of nonmonotonous dependencies of the slopes of the corrosion-fatigue curves for the strained near-a Ti-5Al-2V alloy on the recrystallization annealing temperature has been observed.

cond-mat.mtrl-sci↗