Searcharxiv⌕ Search

arXiv subjects

M. K. Chegurov

Publications and source records attributed to M. K. Chegurov.

7 recordsLinked to original sources

Localized corrosion resistance of ultrafine-grained austenitic steel 321 obtained by Rotary Swaging: The role of annealing conditions

The object of this study was austenitic steel 321, which has an ultrafine-grained (UFG) structure formed by Rotary Swaging (RS). RS leads to the formation of a two-phase macroscopically heterogeneous and, at the same time, a microscopically homogeneous UFG structure with an increased content of martensite. It has been shown that secondary TiC nanoparticles form in the annealing at 450-550C, the reverse transformation of martensite into austenite occurs at 550-650C, and recrystallization begins at 700C. Electrochemical studies of the resistance of the UFG steel to general corrosion, intergranular corrosion (IGC), and pitting corrosion (PC) have been carried out. It has been shown that the UFG steel after RS has a reduced IGC resistance. The surface of steel rods after RS has a reduced hardness and corrosion resistance compared to the central part of the rods. It has been shown that in the temperature range of 450-550C, there is a slight increase in the microhardness, and a significant decrease in the IGC and PC resistance of the UFG steel. Recrystallization at 700-800C leads to an increased PC resistance and IGC resistance. Annealing conditions have been determined that ensure a good combination of strength, ductility and corrosion resistance of the UFG steel. It was demonstrated that to explain the non-monotonic variation in the localized corrosion rate of UFG steel during annealing, it is necessary to consider not only the well-known effects of martensite and delta-ferrite, but also the precipitation of TiC particles and the changes in the free energy of non-equilibrium grain boundaries.

cond-mat.mtrl-sci↗

Effect of superplastic deformation on the intergranular corrosion resistance of austenitic steel 321 with different types of UFG structure: A case of homogeneous and heterogeneous microstructure obtained by ECAP

The effects of superplasticity (SP) on the structure, hardness, and intergranular corrosion (IGC) resistance of UFG 321L steel are reported. By increasing the number of the ECAP cycles (N) and varying the ECAP temperature, and annealing temperature, the degree of the microstructural heterogeneity was changed. Regardless of the microstructural homogeneity degree, UFG steels demonstrated the possibility of realizing the SP effect at temperatures below the onset temperature of dynamic recrystallization. The dependence of ductility of the UFG steel on the test temperature is non-monotonic with a minimum at 450-600C. The maximum elongation to failure (~250%) was achieved at a SP temperature of 800C. The SP deformation of the UFG steel is controlled by the power law creep. It is shown that the hardness of UFG steel samples after SP is equal than the hardness of UFG steels annealed at the same temperature. It is also shown what SP leads to a decrease in the IGC resistance of the UFG steel. Heterostructured steel have reduced ductility, as well as lower resistance to IGC after tension tests at room temperature (RT). The minimum IGC resistance is ensured at N=2, and the maximum - at N=4. The IGC resistance of homogeneous UFG samples after tension testing exceeds the IGC resistance of coarse-grained steel. Tension test at a RT has the greatest negative effect on the IGC resistance of heterostructured steel, and the least negative effect on the IGC resistance of homogeneous steel. Increasing the number of ECAP cycles enhances the ductility of the UFG steel at 750-900C. Increasing the ECAP temperature results in a simultaneous decrease in ductility and flow stress. Heterostructured steel exhibits minimal values of the activation energy of SP deformation. Increasing the number of ECAP cycles and increasing the ECAP temperature lead to an increase in the activation energy of SP deformation.

cond-mat.mtrl-sci↗

Effect of severe plastic deformation realized by rotary swaging on the mechanical properties and corrosion resistance of near-a-titanium alloy Ti-2.5Al-2.6Zr

The research aims to analyze the impact that severe plastic deformation arising during Rotary Swaging has on mechanical properties and corrosion resistance of a near-a-titanium alloy Ti-2.5Al-2.6Zr (Russian industrial name PT7M). The nature of corrosion decay in fine-grained alloys caused by hot salt corrosion is known to vary from pit corrosion to intercrystalline corrosion at the onset of recrystallization processes. Resistance to hot salt corrosion in a fine-grained titanium alloy Ti-2.5Al-2.6Zr is shown to depend on the structural-phase state of grain boundaries that varies during their migration as a result of covering corrosive doping elements (aluminum, zirconium) distributed in the crystal lattice of a titanium alloy.

cond-mat.mtrl-sci↗

Effect of the Sc/Zr ratio on the corrosion resistance of Al-Mg cast alloys

The results of investigations of the corrosion resistance of Al-Mg-Sc-Zr alloys with varying Mg content and different Sc/Zr ratios are presented. The objects of investigations were the Al-Mg-Sc-Zr alloys with total Sc + Zr content of 0.32 wt%. The concentration of Sc and Zr in the alloys varied with the increments of 0.02 wt%. The alloys were produced by induction casting. The effect of annealing temperature on the microhardness and electrical resistivity of the Al-Mg-Sc-Zr alloys was investigated. Corrosion tests were carried out in a medium simulating intergranular corrosion in aluminum alloys. Electrochemical studies and mass loss tests were performed. An increase in the Sc concentration and a decrease in the Zr one were shown to result in an increase in the corrosion rate. The primary Al3(ScxZr1-x) particles were found to have the main effect on the corrosion resistance of Al-Mg-Sc-Zr alloys. The dependence of the corrosion current on the annealing temperature of the Al-Mg-Sc-Zr alloy was found to have a non-monotonous character (with a maximum).

cond-mat.mtrl-sci↗

Superplasticity-like behavior of ultrafine-grained austenitic steel 321

Hot rolled commercial metastable austenitic steel 321 with strongly elongated thin delta-ferrite particles in its microstructure was the object of investigations. Ultrafine-grained (UFG) microstructure in steel 321 was formed by Equal Channel Angular Pressing (ECAP) at 150 oC and 450 oC. When heating the UFG steel specimens, the nucleation of sigma-phase particles blocking the grain boundary migration was observed. The maximum elongation to failure (~250%) was achieved at the deformation temperature 750 oC. The process of superplastic deformation of the UFG steel 321 is controlled by simultaneous grain boundary sliding and power-law creep. The contribution of each process depends on the grain growth rate in the superplasticity regime as well as on defect accumulation on the grain boundaries. The fracture of the UFG steel 321 specimens has a cavitational character - an intensive formation of large elongated pores at the non-metallic particles as well as of the submicron pores at the sigma-phase particles in the course of superplastic deformation were observed.

cond-mat.mtrl-sci↗

Microstructure Thermal Stability and Superplastic Behavior of Al-6%Mg-0.12%Sc-0.10%Zr-0.10%(Yb, Er, Hf) Ultrafine-Grained Alloys

Superplastic behavior of ultrafine-grained (UFG) Al-6Mg-0.12Sc-0.10Zr-0.1X alloys, where X = Yb (Alloy #1-Yb), Er (Alloy #2-Er), and Hf (Alloy #3-Hf), has been studied. The total content of Sc, Zr, Yb, Er, Hf in the alloys was 0.32 wt.% (0.117-0.118 at.%). The alloys used for benchmarking were Al-6Mg-0.12Sc-0.20Zr (Alloy #4-Zr) and Al-6Mg-0.22Sc-0.10Zr (Alloy #5-Sc). Their UFG microstructure was formed with ECAP. Two different types of deformation behavior during superplasticity were demonstrated. A simultaneous increase in yield stress and elongation to failure during superplastic deformation was discovered. High deformation temperatures were shown to cause a competition between dynamic (strain-induced) grain growth and dynamic recrystallization, leading to a finer grain microstructure. The values of strain hardening factor (n), strain rate sensitivity factor (m), and superplastic deformation threshold stress (Sp) were determined. The impact of the type and concentration of alloying elements on the deformation behavior and dynamic grain growth of Al-6%Mg alloys was investigated. It was established that the maximum elongation to failure in Alloy #1-Yb and Alloy #2-Er is observed at lower deformation temperatures than in Alloy #4-Zr and Alloy #5-Sc. The superplastic properties of Alloy #3-Hf are superior to those of Alloy #4-Zr and Alloy #5-Sc with high content of alloying elements (in at.%). Alloy #1-Yb manifests good elongation to failure (910%) at low temperatures (400 oC). The satisfiability of Hart's criterion for calculating uniform deformation value under superplastic conditions was verified. It was demonstrated that cavitation when pores are formed in large Al3X particles at high temperatures causes early failure of aluminum alloys.

cond-mat.mtrl-sci↗

Effect of ECAP and heat treatment on mechanical properties, stress relaxation behavior and corrosion resistance of a 321-type austenitic steel with increased delta-ferrite content

Hot rolled commercial metastable austenitic steel 0.8C-18Cr-10Ni-0.1Ti (Russian industrial name 08X18H10T, analog 321L) with strongly elongated thin delta-ferrite particles in its microstructure was the object of investigations. The lengths of these delta-particles were up to 500 mkm, the thickness was 10 mkm. The formation of the strain-induced martensite as well as the grinding of the austenite and of the delta-ferrite grains take place during ECAP. During the annealing of the UFG steel, the formation of the delta-phase particles takes place. These particles affect the grain boundary migration and the strength of the steel. However, a reduction of the Hall-Petch coefficient as compared to the coarse-grained (CG) steel due to the fragmentation of the delta-ferrite particles was observed. The samples of the UFG steel were found to have 2-3 times higher stress relaxation resistance as compared to the CG steel (a higher macroelasticity stress and a lower stress relaxation magnitude). The differences in the stress relaxation resistance of the UFG and CG steels were investigated. ECAP was shown to result in an increase in the corrosion rate and in an increased tendency to the intergranular corrosion (IGC). The reduction of the corrosion resistance of the UFG steel was found to originate from the increase in the fraction of the strain-induced martensite during ECAP.

cond-mat.mtrl-sci↗