The study of the efficiency of nitrogen to NV-center conversion in high nitrogen content samples

The nitrogen-vacancy color center in diamond is one of the most important systems in the fast-growing field of sensing. This color centers are used in both high-resolution and high-sensitivity sensors. However, techniques for quick and efficient formations of this color center are still in the development stage. In this paper, we present a study on the influence of the electron irradiation dose on the conversion of substitutional nitrogen into $\text{N}{\text{V}^{-}}$ centers. The study was done on diamonds that were highly enriched with nitrogen (~100 ppm), which on one hand should maximize the effect of irradiation, and on another be of interest for high-sensitivity magnetometers. The maximum achieved conversion efficiency was as high as ${37\pm 3.7}$, with no observed saturation on the electron dose even with the simplest annealing procedure. The measurements of the corresponding dephasing time made it possible to estimate for shot-noise limited sensitivity per unit volume of a stationary field sensor with such a diamond to be ${9\pm 1\times {{10}^{-14}}\text{T}}/{\sqrt{\text{Hz}\cdot \text{m}{\text{m}^{-3}}}}\;$.

cond-mat.mtrl-sci

All-diamond optical assemblies for a beam-multiplexing X-ray monochromator at the Linac Coherent Light Source

A double-crystal diamond (111) monochromator recently implemented at the Linac Coherent Light Source (LCLS) enables splitting of the primary X-ray beam into a pink (transmitted) and a monochromatic (reflected) branch. The first monochromator crystal with a thickness of 100 um provides sufficient X-ray transmittance to enable simultaneous operation of two beamlines. Here we report on the design, fabrication, and X-ray characterization of the first and second (300-um-thick) crystals utilized in the monochromator and the optical assemblies holding these crystals. Each crystal plate has a region of about 5 X 2 mm2 with low defect concentration, sufficient for use in X-ray optics at the LCLS. The optical assemblies holding the crystals were designed to provide mounting on a rigid substrate and to minimize mounting-induced crystal strain. The induced strain was evaluated using double-crystal X-ray topography and was found to be small over the 5 X 2 mm2 working regions of the crystals.

physics.optics

Behaviour of muonium in synthetic diamond

The probabilities of finding the muon in various states in synthetic single crystal and polycrystalline diamond were studied. In the IIa-type single-crystal sample at 150 K the contributions of the diamagnetic muon, `normal', and `anomalous' muonium were observed to be 1.5 %, 57 % and 8.1 %, respectively. The missing fraction of muon polarization was 33.4 %, which is approximately two times smaller than in the Ia-type natural diamond, and two or three times greater than in the IIa- and IIb-type natural diamonds. The muon spin relaxation rates at the `normal' and `anomalous' muonium states in the synthetic and natural samples of IIa- and IIb-type are similar.