Impact of Carbon Contamination on the Low-Temperature Electric Conduction of the Spark-Plasma Sintered Barium Titanate Ceramics

The dielectric and electric conduction properties of BaTiO3 samples fabricated by the spark plasma sintering with additional contamination by different content of carbon have been investigated in the temperature range from 77 through 408 K in small non-heating electric fields and in the range of 77 - 200K under strong electric fields up to 20 kV/cm. The effective dielectric permittivity of the samples with additional carbon achieves colossal values at low frequency, up to several units per 106 at 393 K. In the low temperature range, it remains very high magnitude, 10^4 -10^5 at low frequency and is strongly dependent on the carbon content. The electric conduction in the range of 77 - 200 K bears the hopping conduction and obeys the Mott law. We also studied electric conduction and effective dielectric permittivity vs electric field strength in the range of 77 - 200 K. The results are explained within the frames of hopping conduction theory and suggestion on different constituents in polarization processes and electric conduction.

cond-mat.mtrl-sci

Influence of BaTiO_3 nanoparticles on the anisotropy of the dielectric properties of nematic liquid crystal 5CB

This work is devoted to the mechanisms of dielectric response and electric conductivity of suspensions consisting of the nematic liquid crystal 5CB with different concentrations (from 0 to 10 wt.%) of ferroelectric BaTiO_3 nanoparticles with an average size of 24 nm. We revealed that the incorporation of nanoparticles influences significantly the dielectric permittivity magnitude and anisotropy, as well as dielectric losses of the suspension. A pronounced temperature dependence of the anisotropic dielectric permittivity of the suspensions was found at lower temperatures corresponding to the mesophase state; but it is also present at higher temperatures corresponding to the isophase. The dependence of the mesophase-isophase transition temperature on the concentration of BaTiO_3 nanoparticles appeared nonmonotonic. With increasing temperature, both the capacitance and the electrical resistance of the pure liquid crystal increase, as well as it increases in the suspensions with small concentration of BaTiO_3 nanoparticles. Due to space charge accumulation in the shells of nanoparticles, larger concentrations of BaTiO_3 nanoparticles influence strongly the ionic transport by promoting the formation of ionic-electronic screening. This effect modifies the dielectric properties and conduction mechanisms of the suspension, leading to the nonmonotonic dependence of the mesophase - isophase transition temperature versus the nanoparticle concentration.

cond-mat.mtrl-sci

Electric Charge Transport and Dielectric Properties of the Barium Titanate Ceramics Obtained by Spark-Plasma Sintering with Different Carbon Content

Barium titanate (BaTiO3) ceramics with a different content of carbon were synthesized by spark-plasma sintering (SPS) at the temperature of 1100 C in vacuum under pressure. The concentration and distribution of carbon impurity inside the samples is estimated by scanning electron microscopy (SEM). The resistivity vs temperature and electric field dependences of the SPS ceramics with different carbon concentration have been studied. It is shown that their conduction is determined by the variable range hopping mechanism and obeys the Mott law. The density of localized states and localization radius of the electron wave function are determined. The difference in low-temperature resistivity of the SPS ceramics is caused by carbon concentration and connected with it variation of the dielectric permittivity. The relative dielectric permittivity of the SPS ceramics is colossal and reaches the values of 10^5 - 10^6 order. The larger carbon concentration is, the smaller the permittivity and resistivity are within the Mott hopping conduction temperature range. In the range from 250 K to 408 K one observes that the dielectric permittivity strongly increases forming a maximum in all samples, which may be related to the phase transition. Along with this, resistivity manifests a simultaneous sharp decrease. The decrease of resistivity along with the characteristic dependence of resistivity vs dielectric permittivity in the Mott conduction temperature range, evidences the validity of Heywang model for the description of SPS ceramics conduction mechanisms. The resistivity strongly decreases with increasing frequency in the AC regime, which agrees both with models of hopping conduction and effects based on the Maxwell-Wagner model. The studied SPS BaTiO3 ceramics are attractive for applications in energy storage and sensorics.

cond-mat.mtrl-sci

Colossal dielectric response of HfxZr1-xO2 nanoparticles

We reveal a colossal dielectric response of small (5 - 10 nm) oxygen-deficient HfxZr1-xO2 nanoparticles (x = 1 - 0.4), prepared by the solid-state organonitrate synthesis. The effective dielectric permittivity of the pressed HfxZr1-xO2 nanopowders has a pronounced maximum at 38 - 88 C, which shape can be fitted by the Curie-Weiss type dependence modified for the diffuse ferroelectric-paraelectric phase transition. The maximal value of the dielectric permittivity increases from 1.5*10^3 (for x = 1) to 1.5*10^5 (for x= 0.4) at low frequencies (~4 Hz); being much smaller, namely changing from 7 (for x = 1) to 20 (for x = 0.4) at high frequencies (~500 kHz). The frequency dispersion of the dielectric permittivity maximum position is almost absent, meanwhile the shape and width of the maximum changes in a complex way with increase in frequency. The temperature dependencies of the dielectric permittivity and resistivity are almost mirror-like turned over in respect to each other, which means that all their features, such as position and shape of maxima, plateau, minima and inflexions, almost coincide after the mirror reflection in respect to the temperature axis. These correlations of resistivity and dielectric permittivity are well-described in the Heywang barrier model applied together with the variable range hopping conduction model in semiconducting ferroelectrics. The ferroelectric-like behavior of the small oxygen-deficient HfxZr1-xO2 nanoparticles is expected from the Landau-Ginzburg-Devonshire approach and density functional theory calculations. Obtained results may be useful for developing silicon-compatible functional nanomaterials based on HfxZr1-xO2 nanoparticles.

cond-mat.mtrl-sci

Dynamics of charge states at the surface of a ferroelectric nanoparticle in a liquid crystal

The liquid crystal with suspended ferroelectric nanoparticles is an interesting object for fundamental research of the long-range dipole-dipole interactions; as well as it is promising for optical, optoelectronic and electrochemical applications. Such suspensions can serve as basic elements for advanced nonvolatile memory cells and energy storage devices. The work studies the cells filled with a nematic liquid crystal 5CB and the cells containing 5CB with 0.5 wt.% and 1 wt.% of BaTiO3 nanoparticles with an average size of 24 nm. We analyzed the time dependences of the current flowing through the cells at constant applied voltage and the voltage dynamics in the no-load mode. The time dependences of the current and voltage show a slowing down decay rate. For the cells with BaTiO3 nanoparticles, the decrease in the decay time is characteristic. A possible physical reason for the retarding decay time rate is the indirect effect of screening charges, which cover ferroelectric nanoparticles, and slow ionic transport in the liquid crystal. To explain the dynamics of current and voltage, the finite element modeling of the polarization distribution, domain structure dynamics, and charge state of nanoparticles in a liquid crystal is performed using Landau-Ginzburg-Devonshire approach. Theoretical results confirmed the leading role of screening charges, because the surface of a ferroelectric nanoparticle adsorbs an ionic-electronic charge that partially screens its spontaneous polarization in single-domain and/or poly-domain states. When an electric field is applied to the liquid crystal with nanoparticles, it can release part of the screening charge (mainly due to the change in the polarization of the nanoparticle), which will lead to a decrease in decay time rate of the current and voltage dependences.

cond-mat.mtrl-sci

Interfacial Effects and Negative Capacitance State in P(VDF-TrFE) Films with BaTiO3 Nanoparticles

We analyze the temperature dependences of the effective dielectric permittivity of P(VDF-TrFE) films with BaTiO3 nanoparticles (with the average size 24 nm). Transition from a weak to a strong nonlinear temperature dependence of the dielectric permittivity is observed near the freezing temperature (near -50 °C) of P(VDF-TrFE). The transition is followed by a diffuse step-like change in the temperature range (0 - 40)°C, and a subsequent maximum of the dielectric permittivity in the P(VDF-TrFE) films with a lower content (~20-40 vol.%) of BaTiO3 nanoparticles; or by a quasi-plateau of the dielectric permittivity in the P(VDF-TrFE) films with a higher content (~ 50-70 vol.%) of BaTiO3 nanoparticles. The frequency dispersion of the dielectric permittivity is significant in the vicinity of its maxima. The temperature-frequency shift of the permittivity region with a strong temperature dependence is positive. The temperature-frequency shift of the maxima is insignificant (or negative) for the P(VDF-TrFE) films with lower content of BaTiO3 nanoparticles. Increasing the content of BaTiO3 nanoparticles leads to a significant increase in the relative dielectric permittivity of the P(VDF-TrFE)-BaTiO3 films compared to pure P(VDF-TrFE) films (from 8 to 50 at 25 °C). At the same time, the voltage response of the studied P(VDF-TrFE)/BaTiO3 films to the frequency-modulated IR radiation flux has rather photoelectric than pyroelectric nature. A phenomenological model, which considers the screening charges at the interfaces, as well as dipole-dipole cross-interaction effects between the ferroelectric nanoparticles, is proposed to describe the temperature and frequency behavior of the effective dielectric permittivity. The negative capacitance state, which originates due to the interfacial effects, is predicted in the P(VDF-TrFE) films with a high content of BaTiO3 nanoparticles.

cond-mat.mtrl-sci

Anomalous Behavior of the Dielectric and Pyroelectric Responses of Ferroelectric Fine-Grained Ceramics

We revealed the anomalous temperature behavior of the giant dielectric permittivity and unusual frequency dependences of the pyroelectric response of the fine-grained ceramics prepared by the spark plasma sintering of the ferroelectric BaTiO3 nanoparticles. The temperature dependences of the electro-resistivity indicate the frequency-dependent transition in the electro-transport mechanisms between the lower and higher conductivity states accompanied by the maximum in the temperature dependence of the loss angle tangent. The pyroelectric thermal-wave probing revealed the existence of the spatially inhomogeneous counter-polarized ferroelectric state at the opposite surfaces of the ceramic sample. We described the temperature behavior of the giant dielectric response and losses using the core-shell model for ceramic grains, effective medium approach and Maxwell-Wagner approach. The superparaelectric-like state with a giant dielectric response may appear due to the internal barrier-layer capacitance effect, while the step-like thermal activation of localized polarons in the semiconducting grains is not excluded. The elucidation of the state microscopic origin requires measurements in the frequency range above 1 MHz.

cond-mat.mtrl-sci

Ferroelectric Nanoparticles in Liquid Crystals: The Role of Ionic Transport at Small Concentrations of the Nanoparticles

We reveal the visible influence of the ultra-small concentrations (1 wt.% or less) of the BaTiO3 nanoparticles (average size 24 nm) on the current-voltage characteristics and capacitance of the dielectric liquid crystal (LC) 5CB. The pure LC cell demonstrates higher current (and thus smaller resistance) than the LC cells filled with a very small concentration (0.5-1) wt.% of BTO nanoparticles. The same trend is observed for the charge-voltage characteristics: the capacitance loop is the widest for the pure LC cell and becomes noticeably thinner in the presence of (0.5-1) wt.% of BaTiO3 nanoparticles. This seems counterintuitive, because 1 wt.% of ferroelectric nanoparticles very slightly modify the effective dielectric response and should not influence on the director distribution and elastic properties of the LC. We conclude that a possible physical reason of this observation is the influence of the ionic-electronic screening charges, which cover the ferroelectric nanoparticles and become polarized in the external field, on the ionic transport in the LC.

cond-mat.mtrl-sci

Induced smectic ordering and blue phase formation in mixtures of cyanobiphenyls and cholesterol esters

It has been found that in mixtures of nematic E7 and smectogenic cholesteryl oleyl carbonate (COC) the S$_A$-N* transition temperature is substantially (by ~20 K) increased, as compared with pure COC, at E7 concentrations around ~40%. Within the same concentration range, the isotropic transition is preceded by formation of blue phase, with its maximum width of ~3.5 K clearly correlated to the increased thermal stability of the S$_A$ phase. With other cholesterol esters or cyanobiphenyls (cholesteryl nonanoate, 5CB), this effect was either much weaker or not observed. No enhancement of smectic phase was noted when E7 was replaced by N$_{tb}$-forming nematic mixture based on CB7CB with two cyanobiphenyl moieties. Selective Bragg reflection of light (BRL) spectra were measured in all three temperature regions, including the unwinding of the cholesteric helix on cooling towards S$_A$ phase and characteristic selective BRL changes in the blue phase. In the latter case, the measured λ$_{max}$ values were dependent both on the helical twisting power in the cholesteric phase and on the lattice size and orientation in the blue phase. Also considered were the effects of ferroelectric BaTiO$_3$ nanoparticles accumulated at disclination lines upon the blue phase thermal stability.

cond-mat.soft