SearcharxivSearch

arXiv subjects

Stephanie Girod

Publications and source records attributed to Stephanie Girod.

2 recordsLinked to original sources

Solution-Based Fabrication of High-Performance K$_{0.5}$Na$_{0.5}$NbO$_3$ Thin Films for Surface Haptics

K$_{0.5}$Na$_{0.5}$NbO$_3$ is among the most promising lead-free piezoelectrics. While its sputtered films match the performance of the champion piezoelectric Pb(Zr,Ti)O$_3$, reproducible processing of high-quality and time-stable solution-processed K$_{0.5}$Na$_{0.5}$NbO$_3$ films remains challenging. Here, we report 1 $\mu$m-thick Mn-doped K$_{0.5}$Na$_{0.5}$NbO$_3$ films prepared through a chemical solution deposition process, which have perfectly dense microstructure and uniform composition across their thickness. The films exhibit a high transverse piezoelectric coefficient ($e_{31,f} = -15.4$ C/m$^2$), high dielectric permittivity ($\varepsilon_r \approx 920$), low dielectric losses ($\tan\delta = 0.05$) and can withstand electric fields up to at least 1 MV/cm. The functional properties show excellent stability over time, and the synthesis process is reproducible. Furthermore, a surface acoustic haptic device is demonstrated by using K$_{0.5}$Na$_{0.5}$NbO$_3$ thin-film actuators. The results demonstrate the high potential of Mn-doped K$_{0.5}$Na$_{0.5}$NbO$_3$ films to become a replacement for lead-based Pb(Zr,Ti)O$_3$ films in piezoelectric applications.

cond-mat.mtrl-sci

Crystallization of piezoceramic films on glass via flash lamp annealing

Integration of thin-film oxide piezoelectrics on glass is imperative for the next generation of transparent electronics to attain sensing and actuating functions. However, their crystallization temperature (above 650 °C) is incompatible with most glasses. We developed a flash lamp process for growth of piezoelectric lead zirconate titanate films. The process enables crystallization on various types of glasses in a few seconds only. Functional properties of these films are comparable to the films processed with standard rapid thermal annealing at 700 °C. A surface haptic device was fabricated with a 1 $\unicode{x00B5}$m-thick film (piezoelectric e$_{33,f}$ of -5 C m$^{-2}$). Its ultrasonic surface deflection reached 1.5 $\unicode{x00B5}$m at 60 V, sufficient for its use in surface rendering applications. This flash lamp annealing process is compatible with large glass sheets and roll-to-roll processing and has the potential to significantly expand the applications of piezoelectric devices on glass.

physics.app-ph