TY - RPRT TI - In situ $He^{+}$ irradiation of the double solid solution $(Ti_{0.5},Zr_{0.5})_{2}(Al_{0.5},Sn_{0.5})C$ MAX phase: Defect evolution in the 350-800 °C temperature range AU - B. Tunca AU - G. Greaves AU - J. A. Hinks AU - P. O. Å. Persson AU - J. Vleugels AU - K. Lambrinou PY - 2021 DO - 10.1016/j.actamat.2020.116606 UR - https://arxiv.org/abs/2101.04981 ID - 2101.04981 ER -