arXiv · 1404.0428
Thermoelectric properties of Sr0.61Ba0.39Nb2O6-{\delta} ceramics annealed in different oxygen-reduction conditions
Abstract
The thermoelectric properties of Sr0.61Ba0.39Nb2O6 ceramics, reduced in different conditions, were investigated in the temperature region from 323 K to 1073 K. The electrical transport behaviors of the samples are dominated by the thermal-activated polaron hopping, the Fermi glass behavior, and the Anderson localized behavior from low temperatures to high temperatures, respectively. The lattice thermal conductivity presents a plateau at high temperatures, indicating a glass-like thermal conduction behavior. Both the thermoelectric power factor and the thermal conductivity increase with the increasing degree of oxygen-reduction. Taking these two factors into account, the oxygen-reduction can still contribute to promoting the thermoelectric figure of merit. The highest ZT value (~0.19 at 1073 K) is obtained in the heaviest oxygen reduced sample.
Explore related subjects
Keep this discovery
Y. Li, J. Liu, C. L. Wang, W. B. Su, Y. H. Zhu, J. C. Li, L. M. Mei. 2014-04-02. Thermoelectric properties of Sr0.61Ba0.39Nb2O6-{\delta} ceramics annealed in different oxygen-reduction conditions. https://doi.org/10.1088/1674-1056/24/4/047201
Cite the original work for its findings. Save a collection to share your selection of sources.