Thickness and temperature dependence of the magnetodynamic damping of pulsed laser deposited $\text{La}_{0.7}\text{Sr}_{0.3}\text{MnO}_3$ on (111)-oriented SrTi$\text{O}_3$
Abstract
We have investigated the magnetodynamic properties of $\text{La}_{0.7}\text{Sr}_{0.3}\text{MnO}_3$ (LSMO) films of thickness 10, 15 and 30 nm grown on (111)-oriented SrTi$\text{O}_3$ (STO) substrates by pulsed laser deposition. Ferromagnetic resonance (FMR) experiments were performed in the temperature range 100--300 K, and the magnetodynamic damping parameter $α$ was extracted as a function of both film thickness and temperature. We found that the damping is lowest for the intermediate film thickness of 15 nm with $α\approx 2 \cdot 10^{-3}$, where $α$ is relatively constant as a function of temperature well below the Curie temperature of the respective films.
Explore related subjects
Keep this discovery
Vegard Flovik, Ferran Macià, Sergi Lendínez, Joan Manel Hernàndez, Ingrid Hallsteinsen, Thomas Tybell, Erik Wahlström. 2016-07-16. Thickness and temperature dependence of the magnetodynamic damping of pulsed laser deposited $\text{La}_{0.7}\text{Sr}_{0.3}\text{MnO}_3$ on (111)-oriented SrTi$\text{O}_3$. https://doi.org/10.1016/j.jmmm.2016.07.028
Cite the original work for its findings. Save a collection to share your selection of sources.