Phonon-driven ultrafast symmetry lowering in a Bi$_2$Se$_3$ crystal

Abstract

Selective excitation of coherent high-amplitude vibrations of atoms in a solid can induce exotic nonequilibrium states, in which the character of interactions between electronic, magnetic and lattice degrees of freedom is considerably altered and the underlying symmetries are broken. Here we use intense single-cycle terahertz pulses to drive coherently the dipole-active $E_u^1$ phonon mode of a Bi$_2$Se$_3$ crystal. As a result, several Raman-active modes are simultaneously excited in a nonlinear process, while one of them, having the $E_g^2$ symmetry, experiences dynamical splitting during the first two picoseconds after excitation. The corresponding angular scattering pattern is modified indicating coexistence of two phonon modes characteristic of a nonequilibrium state with a lower crystal symmetry. We observe also a short-lived frequency splitting of the original $E_g^2$ mode that immediately after excitation amounts to $\sim 25\%$ of the unperturbed value. This transient state relaxes with a characteristic time of $\sim$ 1 ps, that is close to the decay time of the squared amplitude of the resonantly excited infrared-active $E_u^1$ mode. We discuss possible mechanisms of the dynamical splitting: nonlinear lattice deformation caused by the intense $E_u^1$ vibrations and excitation of anisotropic electronic distribution due to nonlinear electron-phonon interaction. Our data also contain an evidence in favor of the sum-frequency Raman mechanism of generation of the coherent $E_g^2$ phonons in Bi$_2$Se$_3$ excited by terahertz pulses.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

A. A. Melnikov, Yu. G. Selivanov, S. V. Chekalin. 2020-12-07. Phonon-driven ultrafast symmetry lowering in a Bi$_2$Se$_3$ crystal. https://doi.org/10.1103/physrevb.102.224301

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.

cond-mat.mtrl-sci