Plastic deformation of the CaMg$_{2}$ C14-Laves phase from 50-250$^\circ$C
Abstract
Intermetallic phases can significantly improve the creep resistance of magnesium alloys, extending their use to higher temperatures. However, little is known about the deformation behaviour of these phases at application temperatures, which are commonly below their macroscopic brittle-to-ductile-transition temperature. In this study, we therefore investigate the activation of different slip systems of the CaMg$_2$ phase and the occurrence of serrated yielding in the temperature range from 50$^\circ$C to 250$^\circ$C. A decreasing amount of serrated flow with increasing temperature suggests that solute atoms govern the flow behaviour when the CaMg$_{2}$ phase is off-stoichiometric.
Explore related subjects
Keep this discovery
Martina Freund, Doreen Andre, Christoffer Zehnder, Hanno Rempel, Dennis Gerber, Muhammad Zubair, Stefanie Sandlöbes-Haut, James S. K. -L. Gibson, Sandra Korte-Kerzel. 2021-09-23. Plastic deformation of the CaMg$_{2}$ C14-Laves phase from 50-250$^\circ$C. https://arxiv.org/abs/2109.11367
Cite the original work for its findings. Save a collection to share your selection of sources.