Large perpendicular magnetic anisotropy of transition metal dimers driven by polarization switching of two-dimensional ferroelectric In2Se3 substrate

Abstract

Large perpendicular magnetic anisotropy (MA) is highly desirable for realizing atomic-scale magnetic data storage which represents the ultimate limit of the density of magnetic recording. In this work, we studied the MA of transition metal dimers Co-Os, Co-Co and Os-Os adsorbed on two-dimensional ferroelectric In2Se3 (In2Se3-CoOs, In2Se3-OsCo, In2Se3-CoCo and In2Se3-OsOs) by first-principles calculations. It is found that the Co-Os dimer in In2Se3-CoOs has large total perpendicular magnetic anisotropy energy (MAE) of ~ 40 meV. In particular, the MAE arising from Os atom is up to ~ 60 meV. The large MAE is attributed to the high spin-orbit coupling constant and the onefold coordination of Os atom. In addition, the MA of the dimers can be tuned by the polarization reversal of In2Se3. When the polarization is upward, the easy-axis directions of MA in In2Se3-OsCo, In2Se3-CoCo and In2Se3-OsOs are all in-plane, while the directions become perpendicular as the polarization is switched to downward. For the In2Se3-CoOs, switching polarization from upward to downward enhance the perpendicular MA from ~ 20 meV to ~ 40 meV. Based on the second-order perturbation theory, we confirm that the exchange splitting of dxy/dx2-y2 and dxz/dyz orbitals as well as the occupation of dz2 orbital at the vicinity of Fermi level play important roles in the changes of MA with the reversal of FE polarization of In2Se3.

Explore related subjects

Keep this discovery

BibTeXRIS

Wen Qiao, Deyou Jin, Wenbo Mi, Dunhui Wang, Shiming Yan, Xiaoyong Xu, Tiejun Zhou. 2022-02-28. Large perpendicular magnetic anisotropy of transition metal dimers driven by polarization switching of two-dimensional ferroelectric In2Se3 substrate. https://doi.org/10.1039/d2cp01864k

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.

cond-mat.mtrl-sci