Visible-Light Photocatalytic Degradation of Cresols using Sustainable 3D-Printed Bi4O5I2-Hematite Scaffold

Abstract

In photocatalysis, the reusability limit of catalysts can contribute to secondary pollution, posing ecological risks. Addressing this, the present study explores the integration of additive manufacturing with photocatalysis by decorating Bi$_4$O$_5$I$_2$ onto a 3D-printed hematite scaffold (Bi$_4$O$_5$I$_2$@3DH) for the degradation of cresols. The 3D-printed hematite grid, fabricated via direct ink writing, exhibited excellent rheological behavior ($\tau\gamma = 24$ Pa), allowing precise shape retention. The sintered Bi$_4$O$_5$I$_2$ was subsequently immobilized via a facile dip-coating method. Under optimized conditions, the composite achieved 99.78\% degradation of 20 mg/L p-cresol within 240 min of irradiation. Notably, hematite served as a porous substrate and contributed to photocatalytic activity. Density functional theory simulations with Hubbard correction (DFT+U) indicated an interfacial charge transfer of approximately -0.9 electrons from hematite to Bi$_4$O$_5$I$_2$, confirming a S-scheme heterojunction between hematite and Bi$_4$O$_5$I$_2$ semiconductors, validating experimental observations. The composite demonstrated strong performance across varied water matrices and in the presence of other cresol isomers. It also retained 84.28\% degradation efficiency after 10 cycles, with negligible catalyst leaching. Furthermore, in vitro and in silico ecotoxicity analyses revealed reduced toxicity of the degradation products. The current work presents a novel and scalable strategy, advancing the use of earth-abundant hematite minerals in sustainable environmental remediation.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Akash Rawat, Raphael B. de Oliveira, Tapas Pal, Kleuton Antunes, Guilherme S. L. Fabris, Raphael M. Tromer, Marcelo L. Pereira Junior, Adarsh Singh, Ashok Kumar Gupta, Douglas S. Galvao, Chandra Sekhar Tiwary. 2025-08-18. Visible-Light Photocatalytic Degradation of Cresols using Sustainable 3D-Printed Bi4O5I2-Hematite Scaffold. https://arxiv.org/abs/2508.13248

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Breaking Water at Graphene Defects

Water dissociation at solid surfaces underpins processes ranging from corrosion and catalysis to electrochemistry and photovoltaics. Defects often serve as reactive sites for dissociation, yet how solvation influences water dissociation at such sites remains poorly understood. Here, we use state-of-the-art machine-learned interatomic potentials to explore water dissociation at defective graphene-water interfaces. We show that solvation qualitatively changes the reaction mechanism at a graphene single vacancy (SV), opening pathways that are absent for an isolated water molecule. Whereas the gas-phase process proceeds via a single concerted channel, the solvated SV splits water through two competing pathways: a basic route forming SV-H and OH-(aq), and an acidic route forming SV-OH and H3O+(aq). These lower-barrier pathways produce distinct chemisorbed intermediates that enhance graphene-water adsorption. Accordingly, even a simple carbon vacancy gives rise to unexpectedly rich interfacial chemistry, coupling surface chemistry to interfacial charge and wettability, with implications for carbon functionalization and nanofluidic transport.

physics.chem-ph

Comprehensive Study of L-Menthol and Octanoic Acid as a Hydrophobic Eutectic Solvent

Hydrophobic eutectic solvents (HES) based on natural compounds represent promising green alternatives to conventional solvents. In this work, we investigate the physicochemical, structural, and dynamical properties of an ES formed by L-menthol and octanoic acid using a combined experimental and molecular dynamics simulation approach. Five compositions with molar ratios from 1:3 to 3:1 were studied with molecular dynamics simulation in the temperature range 15 degrees C to 35 degrees C. Experimental measurements of density and viscosity in the temperature range from 5 degrees C to 35 degrees C were complemented with results obtained from MD simulations employing the OPLS force field. Structural analyses based on radial distribution functions and Kirkwood-Buff integrals reveal that the dominant interactions in the mixture are hydrogen bonds between L-menthol and octanoic acid molecules. Dynamic properties, including self-diffusion coefficients and hydrogen-bond lifetimes, indicate that intermolecular hydrogen bonds between the two components are stronger and longer-lived than bonds between identical species. These findings provide molecular-level insight into the structure and transport properties of menthol-based ESs relevant for green solvent applications.

physics.chem-ph

More is not always better: Dissociative photoionization limits the EUV absorbing photacid generator pentafluorophenyl triflate in photolithography

Pentafluorophenyl triflate has been explored as a highly absorbing neutral photoacid generator (PAG) candidate for next generation chemically amplified resists used in extreme ultraviolet (EUV) lithography. Although increased fluorination enhances EUV absorption, this study demonstrates that such an approach does not necessarily improve photoacid generation efficiency. Using photoelectron-photoion coincidence (PEPICO) spectroscopy at the 92 eV photon energy of the EUV scanners in combination with quantum chemical calculations, the dissociative photoionization of pentafluorophenyl triflate was systematically investigated. The photoionization mass spectrum reveals extensive fragmentation, with the parent ion contributing only 3.1 % of the total signal and CF$_3^+$ representing the dominant product ion. Computed appearance energies align well with experimental trends and support a sequential fragmentation pathway involving loss of SO$_2$, CF$_3$, and CO. Crucially, none of the major dissociation channels yield precursors capable of forming triflic acid, the strong photoacid required for efficient deprotection reactions in chemically amplified resists. Combined with previous dissociative electron attachment studies indicating similarly unfavorable fragmentation, the results demonstrate that despite its high EUV absorption cross section, pentafluorophenyl triflate is unsuitable as a PAG for EUV lithography. The findings highlight the importance of understanding fundamental photoionization and electron interaction mechanisms to guide the rational design of next generation high performance EUV photoresists.

physics.chem-ph