Improved Irreversibility Behaviour and Critical Current Density in MgB2-Diamond Nanocomposites
Abstract
MgB2-diamond nanocomposite superconductors have been synthesized by addition of nano-diamond powder. Microstructural analysis shows that the nanocomposite superconductor consists of tightly-packed MgB2 nano-grains (~50-100 nm) with highly-dispersed and uniformly-distributed diamond nanoparticles (~10-20 nm) inside the grains. The Jc-H and Hiir-T characteristics have been significantly improved in this MgB2-diamond nanocomposite, compared to MgB2 bulk materials prepared by other techniques. Also, the Jc value of 1x104 A/cm2 at 20 K and 4 T and the Hirr value of 6.4 T at 20 K have been achieved
Explore related subjects
Keep this discovery
Y. Zhao, X. F. Rui, C. H. Cheng, H. Zhang, P. Munroe, H. M. Zeng, N. Koshizuka, M. Murakami. 2003-02-18. Improved Irreversibility Behaviour and Critical Current Density in MgB2-Diamond Nanocomposites. https://doi.org/10.1063/1.1606884
Cite the original work for its findings. Save a collection to share your selection of sources.