Advantage on Superconductivity of Heavily Boron-Doped (111) Diamond Films
Abstract
The superconductivity transition temperatures Tc(onset) of 11.4 K and Tc(offset) of 7.4 K, which are the highest in diamond at present, are realized on homoepitaxially grown (111) diamond films with a high boron doping concentration of 8.4E21 cm-3 (4.7 atomic percent). Tc values of (111) diamond films are more than twice as high as those of (100) films at the equivalent boron concentration. The Tc of boron-doped (111) diamond increases as the boron content increases up to the maximum incorporated concentration and is agrees with the value estimated using McMillan's equation. The advantageous Tc for (111) diamond films is due to the higher carrier concentration which exceeds its boron concentration.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Hitoshi Umezawa, Tomohiro Takenouchi, Yoshihiko Takano, Kensaku Kobayashi, Masanori Nagao, Isao Sakaguchi, Minoru Tachiki, Takeshi Hatano, Guofang Zhong, Masashi Tachiki, Hiroshi Kawarada. 2005-03-12. Advantage on Superconductivity of Heavily Boron-Doped (111) Diamond Films. https://arxiv.org/abs/cond-mat/0503303
Cite the original work for its findings. Save a collection to share your selection of sources.