Antiferromagnetic Order of the Ru and Gd in Superconducting RuSr2GdCu2O8

Neutron diffraction has been used to study the magnetic order in RuSr{2}GdCu2O8. The Ru moments order antiferromagnetically at T{N}=136(2)K, coincident with the previously reported onset of ferromagnetism. Neighboring spins are antiparallel in all three directions, with a low T moment of 1.18(6) mu {B} along the c-axis. Our measurements put an upper limit of ~0.1 mu{B} to any net zero-field moment, with fields exceeding ~0.4T needed to induce a measurable magnetization. The Gd ions order independently at T{N}=2.50(2)K with the same spin configuration. PACS numbers: 74.72.Jt, 75.25.+z, 74.25.Ha, 75.30.Kz

cond-mat.supr-con↗

Investigation of conduction band structure, electron scattering mechanisms and phase transitions in indium selenide by means of transport measurements under pressure

In this work we report on Hall effect, resistivity and thermopower measurements in n-type indium selenide at room temperature under either hydrostatic and quasi-hydrostatic pressure. Up to 40 kbar (= 4 GPa), the decrease of carrier concentration as the pressure increases is explained through the existence of a subsidiary minimum in the conduction band. This minimum shifts towards lower energies under pressure, with a pressure coefficient of about -105 meV/GPa, and its related impurity level traps electrons as it reaches the band gap and approaches the Fermi level. The pressure value at which the electron trapping starts is shown to depend on the electron concentration at ambient pressure and the dimensionality of the electron gas. At low pressures the electron mobility increases under pressure for both 3D and 2D electrons, the increase rate being higher for 2D electrons, which is shown to be coherent with previous scattering mechanisms models. The phase transition from the semiconductor layered phase to the metallic sodium cloride phase is observed as a drop in resistivity around 105 kbar, but above 40 kbar a sharp nonreversible increase of the carrier concentration is observed, which is attributed to the formation of donor defects as precursors of the phase transition.