Mechanical Loss in Tantala/Silica Dielectric Mirror Coatings
Abstract
Current interferometric gravitational wave detectors use test masses with mirror coatings formed from multiple layers of dielectric materials, most commonly alternating layers of SiO2 (silica) and Ta2O5 (tantala). However, mechanical loss in the Ta2O5/SiO2 coatings may limit the design sensitivity for advanced detectors. We have investigated sources of mechanical loss in the Ta2O5/SiO2 coatings, including loss associated with the coating-substrate interface, with the coating-layer interfaces, and with the bulk material. Our results indicate that the loss is associated with the bulk coating materials and that the loss of Ta2O5 is substantially larger than that of SiO2.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Steven D. Penn, Peter H. Sneddon, Helena Armandula, Joseph C. Betzwieser, Gianpietro Cagnoli, Jordan Camp, D. R. M. Crooks, Martin M. Fejer, Andri M. Gretarsson, Gregory M. Harry, Jim Hough, Scott E. Kittelberger, Michael J. Mortonson, Roger Route, Sheila Rowan, Christophoros C. Vassiliou. 2003-02-24. Mechanical Loss in Tantala/Silica Dielectric Mirror Coatings. https://doi.org/10.1088/0264-9381%2F20%2F13%2F334
Cite the original work for its findings. Save a collection to share your selection of sources.