Effect of crystalline anisotropy on vertical (-201) and (010) beta-Ga2O3 Schottky barrier diodes on EFG single-crystal substrates

Abstract

Vertical (-201) and (010) beta-Ga2O3 Schottky barrier diodes (SBDs) were fabricated on single-crystal substrates grown by edge-defined film-fed growth (EFG) method. High resolution X-ray diffraction (HRXRD) and atomic force microscopy (AFM) confirmed good crystal quality and surface morphology of the substrates. The electrical properties of both devices, including current-voltage (I-V) and capacitance-voltage (C-V) characteristics, were comprehensively measured and compared. The (-201) and (010) SBDs exhibited on-resistances (Ron) of 0.56 and 0.77 m{\Omega}cm2, turn-on voltages (Von) of 1.0 and 1.3 V, Schottky barrier heights (SBH) of 1.05 and 1.20 eV, electron mobilities of 125 and 65 cm2/(Vs), respectively, with a high on-current of ~1.3 kA/cm2 and on/off ratio of ~109. The (010) SBD had a larger Von and SBH than (-201) SBD due to anisotropic surface properties (i.e., surface Fermi level pinning and band bending), as supported by X-ray photoelectron spectroscopy (XPS) measurements. Temperature-dependent I-V also revealed the inhomogeneous nature of the SBH in both devices, where (-201) SBD showed a more uniform SBH distribution. The homogeneous SBH was also extracted: 1.33 eV for (-201) SBD and 1.53 eV for (010) SBD. The reverse leakage current of the devices was well described by the two-step trap-assisted tunneling model and the one-dimensional variable range hopping conduction (1D-VRH) model. The (-201) SBD showed larger leakage current due to its lower SBH and smaller activation energy. These results indicate the crystalline anisotropy of beta-Ga2O3 can affect the electrical properties of vertical SBDs and should be taken into consideration when designing beta-Ga2O3 electronics.

Explore related subjects

Keep this discovery

BibTeXRIS

Houqiang Fu, Hong Chen, Xuanqi Huang, Izak Baranowski, Jossue Montes, Tsung-Han Yang, Yuji Zhao. 2017-12-04. Effect of crystalline anisotropy on vertical (-201) and (010) beta-Ga2O3 Schottky barrier diodes on EFG single-crystal substrates. https://doi.org/10.1109/ted.2018.2841904

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related papers

Measuring chiral phonons

Chiral phonons are quantized vibrations where the atomic motion in a solid breaks improper rotation symmetries. In many cases, chiral phonons possess angular momenta and are therefore selective to circularly polarized light. Both fundamental and applied research efforts on chiral phonons have been gaining increasing attention owing to their importance in a variety of fields including spintronics, spin-selective chemical reactions, thermal transport, quantum information processing and biosensing, where the bi-directional spin-lattice coupling enabled by chiral phonons can be harnessed in new ways, and potentially lead to new functionalities. Thus far, the studies of chiral phonons across diverse materials platforms have evolved largely independently within these fields, but the experimental techniques are often interrelated. In this perspective, we present a detailed description, as well as advantages and disadvantages of the current approaches for experimentally measuring chiral phonons in chiral and achiral materials. We conclude with a discussion of new methods for measuring chiral phonons. Ultimately, this work seeks to offer an experimental guide for systematically investigating the properties of chiral phonons in various materials systems and applications.

cond-mat.mtrl-sci

A model of grain growth in UN integrating molecular dynamics, phase-field modeling, and uncertainty quantification

Grain growth kinetics and grain-boundary (GB) properties in uranium mononitride (UN) are investigated through an integrated multiscale framework combining molecular dynamics (MD), phase-field modeling, and surrogate-assisted uncertainty quantification. MD simulations yield GB energies for 27 symmetric tilt boundaries from 0--2000~K, which are consistent with available DFT values. The average GB energy is nearly temperature-independent below 1000~K and increases at higher temperatures. A mechanistic pore-drag model applied to the only available grain growth dataset for actinide nitrides yields a mobility reduction factor of $s \approx 0.93$--$0.99$, statistically indistinguishable from unity, confirming that pore drag is negligible under the experimental conditions. The intrinsic GB mobility is therefore extracted directly from the effective mobility, yielding $M_0 = 2.05\times10^{-15}$~m$^4$/(J$\cdot$s) and $Q_M = 0.89$~eV. Phase-field simulations conducted from 1500--2000~K confirm normal curvature-driven grain growth, with grain size distributions converging to the Hillert-like form. A surrogate-assisted global sensitivity analysis---combining principal component analysis, Gaussian process regression, and Sobol decomposition---reveals that the mobility prefactor $M_0$ dominates output variance at all times, followed by the activation energy $Q_M$, while the GB energy $\gamma$ contributes minimally. These results establish the first quantitative grain growth framework for UN and identify the reduction of uncertainty in $M_0$ and $Q_M$ as the highest-priority target for future experimental efforts.

cond-mat.mtrl-sci

Silicon Solar Cell Design for >30% Efficiency via Singlet Fission

Singlet fission (SF) materials convert high-energy photons into multiple charge carriers, providing a route to exceed the efficiency limits of single-junction silicon solar cells without many of the complexities of multi-junction tandem designs. Following the first demonstration of an SF-enhanced silicon solar cell in 2025, there is a need to understand how SF materials can be effectively integrated into high-efficiency industrial silicon devices and translated from proof of concept to a manufacturable technology. Using coupled optical and electrical simulations, we assess the efficiency potential of several industrially relevant silicon cell architectures combined with SF materials. Interdigitated back-contact (IBC) cells offer the greatest potential for improvement due to unrestricted front-surface access and can achieve efficiencies exceeding 33%. However, performance is highly sensitive to front-surface passivation quality. Appropriate silicon design, particularly controlled surface doping and fixed interfacial charge, can mitigate recombination losses and relax passivation requirements for ultra-thin exciton-transfer layers.

cond-mat.mtrl-sci